Polymer Property : Thermal Conductivity = 3.26 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.470 W/m-K

@Temperature 686 °C
3.26 BTU-in/hr-ft²-°F

@Temperature 1270 °F
hot face 842°C, cold face 529°C, mean - 686°C
Pyrotek Insural® 140 Insulating Refractory Shapes for Aluminum
Insural® 140 Precast Shapes are designed for the containment of molten aluminum in hot top modules (cross feeder) and trough/launder applications.AdvantagesNear zero expansion avoids gaps at the jo..
Thermal Conductivity 0.470 W/m-K

@Temperature 200 °C
3.26 BTU-in/hr-ft²-°F

@Temperature 392 °F
Pyrotek NAD-11 Structural Insulation Board
NAD-11 is an asbestos-free cement board with excellent electrical properties. It has a high density cement board reinforced with inorganic fibers.ApplicationsCathode support pads Platen insulation ..
Thermal Conductivity 0.470 W/m-K

@Temperature 100 °C
3.26 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1530
3M Dyneon™ CC646/S Custom Compound  (discontinued **)
This compound consists of a mixture of 60% bronze blended with PTFE.Information provided by Dyneon, A 3M Company
Thermal Conductivity 0.470 - 0.570 W/m-K

@Temperature 100 °C
3.26 - 3.96 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 110 C AL Dense Refractory Castable
Description: Because of special addition this coarse castable shows a very good resistance against liquid aluminum metal.Remarks: These values apply to cast products.Information provided by Gouda Vu..
Thermal Conductivity 0.470 - 0.570 W/m-K

@Temperature 100 °C
3.26 - 3.96 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 120 Dense Refractory Castable
Description: A general purpose castable for use up to 1200°C under normal operating conditions. Curon 120 has good thermal shock resistance.Remarks: These values apply to cast products. Also avai..
Thermal Conductivity 0.470 - 0.570 W/m-K

@Temperature 100 °C
3.26 - 3.96 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 120 HS Dense Refractory Castable
Description: This castable has a very good resistance against thermal shocks because of its low thermal expansion. In addition, it has a high strength. Used in incinerators and for tunnel kiln cars...
Thermal Conductivity 0.470 - 0.570 W/m-K

@Temperature 1000 °C
3.26 - 3.96 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Gouda Vuurvast FI 45-12 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Thermal Conductivity 0.470 - 0.570 W/m-K

@Temperature 1260 °C
3.26 - 3.96 BTU-in/hr-ft²-°F

@Temperature 2300 °F
Gouda Vuurvast GOLITE 145 Refractory Insulating Castable
Description: Golite 145 can be used in direct contact with the furnace conditions and combines a high strength with a good thermal insulation.Remarks: These values apply to cast products. Also avail..
Thermal Conductivity 0.470 - 0.570 W/m-K

@Temperature 1370 °C
3.26 - 3.96 BTU-in/hr-ft²-°F

@Temperature 2500 °F
Gouda Vuurvast GOLITE 155 Refractory Insulating Castable
Description: Due to it's high strength at high temperatures, this material can be applied in direct contact with the firing process.Remarks: These values apply to cast products. Also available i..
Thermal Conductivity 0.470 - 0.570 W/m-K

@Temperature 100 °C
3.26 - 3.96 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 130 HRC AL Dense Refractory Castable
Description: Because of special addition this castable is used for the walls above the liquid level in aluminum melting furnaces.Remarks: These values apply to cast products.Information provided by ..
Thermal Conductivity 0.470 - 0.570 W/m-K

@Temperature 100 °C
3.26 - 3.96 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 130 HRC Dense Refractory Castable
Description: A coarse, low iron castable for use up to 1300°C under normal operation conditions, also usable under reducing circumstances. Curon 130 HRC has a good thermal shock resistance becaus..
Thermal Conductivity 0.470 - 0.570 W/m-K

@Temperature 100 °C
3.26 - 3.96 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 130 HRCC RAPID Dense Refractory Castable
Description: An extra coarse, low iron castable for use to 1300°C under normal operation conditions, also usable under reducing circumstances. Curon 130 HRCC RAPID has good thermal shock resistan..
Thermal Conductivity 0.470 W/m-K

@Temperature 982 °C
3.26 BTU-in/hr-ft²-°F

@Temperature 1800 °F
4 pcf
Thermal Ceramics Cerablanket Blanket
Cerablanket is produced from exceptionally pure oxides of alumina and silica using the spinning process. The resultant quality spun fibers have been optimized for high handling strength, with on ave..
Thermal Conductivity 0.470 W/m-K

@Temperature 982 °C
3.26 BTU-in/hr-ft²-°F

@Temperature 1800 °F
4 pcf
Thermal Ceramics Cerachem Blanket
Cerachem Blanket is a 2600°F (1427°C) maximum temperature rated refractory blanket formed from a unique, patented, spun alumina-silica-zirconia fiber. It is specially designed for applications whe..
Thermal Conductivity 0.470 W/m-K

@Temperature 982 °C
3.26 BTU-in/hr-ft²-°F

@Temperature 1800 °F
4 pcf
Thermal Ceramics Cerachrome Blanket
Made from spun alumina-silica-chromia fiber, Cerachrome Blanket is well suited for hot face lining applications where higher temperatures are encountered, such as soaking pit covers, reheat and forg..
Thermal Conductivity 0.470 W/m-K

@Temperature 260 °C
3.26 BTU-in/hr-ft²-°F

@Temperature 500 °F
Thermal Ceramics Kaocrete B Dense Castable
Kaocrete B is a more plastic material than most refractory castables. It is an excellent plastering material, preferred for patching linings and baffles. Recommended only for relatively thin section..
Thermal Conductivity 0.470 W/m-K

@Temperature 982 °C
3.26 BTU-in/hr-ft²-°F

@Temperature 1800 °F
4 pcf
Thermal Ceramics Kaowool S Blanket
Kaowool S Blanket is produced from high quality spun fibers. It is available in a wide variety of densities and sizes, and offers a highly cost effective alternative to Cerablanket with its 2300°F ..