Material Notes:
Description: This castable has a very good resistance against thermal shocks because of its low thermal expansion. In addition, it has a high strength. Used in incinerators and for tunnel kiln cars.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 1.90 - 2.00 g/cc
0.0686 - 0.0723 lb/in³
After drying at 110°C
Particle Size <= 5000 µm
<= 5000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 25.0 - 35.0 MPa

@Temperature 1000 °C
3630 - 5080 psi

@Temperature 1830 °F
Cold Crushing Strength
40.0 - 50.0 MPa

@Temperature 100 °C
5800 - 7250 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.470 - 0.570 W/m-K

@Temperature 100 °C
3.26 - 3.96 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.510 - 0.610 W/m-K

@Temperature 600 °C
3.54 - 4.23 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.550 - 0.650 W/m-K

@Temperature 1000 °C
3.82 - 4.51 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Maximum Service Temperature, Air 1150 °C
2100 °F
Shrinkage -0.800 - 0.200 %

@Temperature 1000 °C
-0.800 - 0.200 %

@Temperature 1830 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 36 %
36 %
SiO2 45 %
45 %
Descriptive Properties Value Comments
ASTM Classification A
Material Consumption per 1 m3 1850 kg
Mixing Water 14-17 liters
per 100 kgs dry material