Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 5.34 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.670 - 0.770 W/m-K

@Temperature 1000 °C
4.65 - 5.34 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Gouda Vuurvast CURON 150 AC Dense Refractory Castable
Description: Curon 150 AC is a coarse castable for use up to 1500°C with a high strength.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Thermal Conductivity 0.670 - 0.770 W/m-K

@Temperature 1300 °C
4.65 - 5.34 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Gouda Vuurvast CURON 150 HS Dense Refractory Castable
Description: Dense refractory castableRemarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information provided by Gouda Vuurvast.
Thermal Conductivity 0.670 - 0.770 W/m-K

@Temperature 600 °C
4.65 - 5.34 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURON 160 HC Dense Refractory Castable
Description: Because of the selection of raw materials, this castable has a high volume stability and keeps its strength up to high temperatures. In addition, Curon 160 HC has an excellent thermal s..
Thermal Conductivity 0.670 - 0.770 W/m-K

@Temperature 600 °C
4.65 - 5.34 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURON 160 HF Dense Refractory Castable
Description: This castable has a high volume stability and keeps its strength up to high temperatures. In addition, Curon 160 HF has an excellent thermal shock resistance. It is largely used in the ..
Thermal Conductivity 0.670 - 0.770 W/m-K

@Temperature 1300 °C
4.65 - 5.34 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Gouda Vuurvast CURON 145 C Dense Refractory Castable
Description: A low carbon castable for use in reducing atmospheres. Curon 145 C has a coarse structure for improved thermal shock resistance.Remarks: These values apply to cast products.Information ..
Thermal Conductivity 0.670 - 0.770 W/m-K

@Temperature 1300 °C
4.65 - 5.34 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Gouda Vuurvast CURON 145 Dense Refractory Castable
Description: Because of the use of pure raw materials, Curon 145 has a low Fe2O3 content. Therefore this castable is widely used in reducing atmospheres.Remarks: These values apply to cast products...
Thermal Conductivity 0.670 - 0.770 W/m-K

@Temperature 100 °C
4.65 - 5.34 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 150 GM Dense Refractory Castable
Description: Curon 150 GM is a gunmix based on sintered bauxite with an excellent thermal shock resistance and is therefore very well suited for burner blocks.Remarks: These values apply to cast pro..
Thermal Conductivity 0.670 - 0.770 W/m-K

@Temperature 600 °C
4.65 - 5.34 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURON 160 HS Dense Refractory Castable
Description: Because of the selection of raw materials, this castable has a high volume stability and a high strength up to high temperatures. In addition, Curon 160 HS has an excellent thermal shoc..
Thermal Conductivity 0.670 - 0.770 W/m-K

@Temperature 600 °C
4.65 - 5.34 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURON 160 HSC Dense Refractory Castable
Description: Curon 160 HSC is a coarse abrasion resistant castable to be used up to 1600°C in reducing conditions.Remarks: These values apply to cast products.Information provided by Gouda Vuurva..