Thermal Conductivity 6.50 - 8.50 W/m-K

@Temperature 600 °C
45.1 - 59.0 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast FLUCON 160 K Dense Self Flowing Refractory Castable
Description: Flucon 160 K is a self-flowing low cement castable based on silicon carbide. This castable is characterized by high strength high abrasion resistance and excellent thermal shock resista..
Thermal Conductivity 6.50 W/m-K

@Temperature -184 °C
45.1 BTU-in/hr-ft²-°F

@Temperature -299 °F
Latrobe MP35N® Alloy
MP35N is a nickel-cobalt base alloy of the Multiphase alloy system that has a unique combination of properties - ultra high strength, toughness, ductility, and outstanding corrosion resistance. The ..
Thermal Conductivity 6.50 - 7.50 W/m-K

@Temperature 600 °C
45.1 - 52.0 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast VIBRON 162 K Sp Dense Vibrating Refractory Silicon Carbide Castable
Vibron 162 K Sp is a low cement castable based on silicon carbide. This castable is characterized by a very good thermal conductivity, a high abrasion resistance and high resistance against oxidatio..
Thermal Conductivity 6.50 W/m-K

@Temperature 1100 °C
45.1 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Gouda Vuurvast SiC 70 Dense Refractory Brick
Description: This type of brick, based on silicon carbide, is because of a very good thermal shock resistance, abrasion resistance and a high thermal conductivity very well suited for waste incinera..