Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 96.0 °C | 205 °F | |
Indium Corp. Indalloy 105 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 96.0 °C | 205 °F | |
Indium Corp. Indalloy 72 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 96.0 °C | 205 °F | |
Indium Corp. Indalloy 74 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 96.0 °C | 205 °F | |
Indium Corp. Indalloy 81 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 96.0 °C | 205 °F | |
Indium Corp. Indalloy 83 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 96.0 °C | 205 °F | |
Indium Corp. Indalloy 85 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 96.0 °C | 205 °F | |
Indium Corp. Indalloy® 42 Bi-Sn-Pb Solder Alloy Bismuth added to achieve a low melting point. Fair wettability.Information provided by the manufacturer, Indium Corporation. |
|||
Solidus | 96.0 °C | 205 °F | |
Indium Corp. Indalloy 49 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 96.0 °C | 205 °F | |
Williams Advanced Alloys WS96 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Solidus | 96.0 °C | 205 °F | |
Indium Corp. Indalloy 39 Bismuth Solder Alloy Low temperature eutectic solder. Can be used on the same metallization as SnPb based solders. Lowest temperature solder pasteInformation Provided by Indium Corporation |