Physical Properties Metric English Comments
Density 9.60 g/cc
0.347 lb/in³
Thermal Properties Metric English Comments
Melting Point 96.0 - 107 °C
205 - 225 °F
Solidus 96.0 °C
205 °F
Liquidus 107 °C
225 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 45 %
45 %
Lead, Pb 35 %
35 %
Tin, Sn 20 %
20 %