Thermal Properties Metric English Comments
Liquidus 170 °C
338 °F
Indium Corp. Indalloy 99 Bismuth-Lead-Tin Solder Alloy
Information Provided by Indium Corporation
Liquidus 170 °C
338 °F
Indium Corp. Indalloy 281-338 Bismuth-Tin Solder Alloy
Information Provided by Indium Corporation
Liquidus 170 °C
338 °F
AIM 40Bi/60Sn Solder for Photonic Packaging
Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials.
Liquidus 170 °C
338 °F
AIM 54Sn/26Pb/20In Solder for Photonic Packaging
Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials.