Thermal Properties | Metric | English | Comments |
---|---|---|---|
Hot Ball Pressure Test | <= 125 °C | <= 257 °F | IEC 60695-10-2 |
SABIC Innovative Plastics Cycoloy® C1200 PC+ABS (Europe-Africa-Middle East) CYCOLOY C1200 is a PC+ABS blend developed to serve extremely demanding applications in a variety of markets while maintaining good processing properties. The combination of superior heat resistance .. |
|||
Hot Ball Pressure Test | <= 125 °C | <= 257 °F | IEC 60695-10-2 |
SABIC Innovative Plastics Lexan® FST9436 PC Copolymer Medium viscosity opaque, low smoke, and OSU 65/65 compliant PC Copolymer |
|||
Hot Ball Pressure Test | >= 125 °C | >= 257 °F | IEC 598-1 |
LG Chemical Lupoy 1200-08 Polycarbonate Resin Description: LUPOY PC 1200-08 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Hot Ball Pressure Test | >= 125 °C | >= 257 °F | IEC 598-1 |
LG Chemical Lupoy 1200-15 Polycarbonate Resin Description: LUPOY PC 1200-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Hot Ball Pressure Test | >= 125 °C | >= 257 °F | IEC 598-1 |
LG Chemical Lupoy 1200-22 Polycarbonate Resin Description: LUPOY PC 1200-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Hot Ball Pressure Test | >= 125 °C | >= 257 °F | IEC 598-1 |
LG Chemical Lupoy 1201-10 Polycarbonate Resin Description: LUPOY PC 1201-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Hot Ball Pressure Test | >= 125 °C | >= 257 °F | IEC 598-1 |
LG Chemical Lupoy 1201-15 Polycarbonate Resin Description: LUPOY PC 1201-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Hot Ball Pressure Test | >= 125 °C | >= 257 °F | IEC 598-1 |
LG Chemical Lupoy 1301-12 Polycarbonate Resin Description: LUPOY PC 1301-12 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Hot Ball Pressure Test | >= 125 °C | >= 257 °F | IEC 598-1 |
LG Chemical Lupoy 1301V-7 Polycarbonate Resin Description: LUPOY PC 1301V-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.. |
|||
Hot Ball Pressure Test | >= 125 °C | >= 257 °F | IEC 598-1 |
LG Chemical Lupoy 1302-05 Polycarbonate Resin Description: LUPOY 1302-5 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main.. |
|||
Hot Ball Pressure Test | >= 125 °C | >= 257 °F | IEC 598-1 |
LG Chemical Lupoy 1302-07 Polycarbonate Resin Description: LUPOY PC 1302-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Hot Ball Pressure Test | >= 125 °C | >= 257 °F | IEC 598-1 |
LG Chemical Lupoy 1303EP-22 Polycarbonate Resin Description: LUPOY PC 1303EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Hot Ball Pressure Test | >= 125 °C | >= 257 °F | IEC 598-1 |
LG Chemical Lupoy NF1005F 03R Polycarbonate Resin Description: LUPOY NF 1005F03R, eco-friendly UL94 V0/1.5 mm, is designed for extrusion products. It combines an excellent physical property balance of heat resistance, transparency and impact streng.. |
|||
Hot Ball Pressure Test | >= 125 °C | >= 257 °F | IEC 598-1 |
LG Chemical Lupoy NF1007F 10R Polycarbonate Resin Description: LUPOY NF 1007F10R, eco-friendly UL94 V0/3.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpar.. |
|||
Hot Ball Pressure Test | >= 125 °C | >= 257 °F | IEC 598-1 |
LG Chemical Lupoy 1201HP-22 Polycarbonate Resin Description: LUPOY PC 1201HP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Hot Ball Pressure Test | >= 125 °C | >= 257 °F | IEC 598-1 |
LG Chemical Lupoy 1300-03 Polycarbonate Resin Description: LUPOY PC 1300-03 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Hot Ball Pressure Test | >= 125 °C | >= 257 °F | IEC 598-1 |
LG Chemical Lupoy 1300-12 Polycarbonate Resin Description: LUPOY PC 1300-12 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Hot Ball Pressure Test | >= 125 °C | >= 257 °F | IEC 598-1 |
LG Chemical Lupoy 1302-10 Polycarbonate Resin Description: LUPOY PC 1302-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Hot Ball Pressure Test | >= 125 °C | >= 257 °F | IEC 598-1 |
LG Chemical Lupoy 1302HP-10 Polycarbonate Resin Description: LUPOY PC 1302HP-10 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics.. |
|||
Hot Ball Pressure Test | <= 125 °C | <= 257 °F | IEC 60695-10-2 |
SABIC Innovative Plastics NORYL PX9406P PPE+HIPS (Asia Pacific) Nonbrominated, nonchlorinated, flame retarded. Improved productivity and reliability. 125dc HDT. UL94 V-0 rated. Electrical applications. |
|||
Hot Ball Pressure Test | 125 °C | 257 °F | IEC 60335-1 |
Styron CALIBREâ„¢ 201-15 Polycarbonate Resin Overview: CALIBREâ„¢ 201-15 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc.. |
|||
Hot Ball Pressure Test | 125 °C | 257 °F | IEC 60335-1 |
Styron CALIBREâ„¢ 201-6 Polycarbonate Resin Overview: CALIBREâ„¢ 201-6 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistance.. |
|||
Hot Ball Pressure Test | 125 °C | 257 °F | IEC 60335-1 |
Styron CALIBREâ„¢ 203-22 Polycarbonate Resin Overview: CALIBREâ„¢ 200-22 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc.. |
|||
Hot Ball Pressure Test | >= 125 °C | >= 257 °F | IEC 60335-1 |
Styron EMERGEâ„¢ 4850-10 Polycarbonate EMERGEâ„¢ 4850-10 advanced resin provides superior ignition resistance and ultraviolet light resistance in opaque applications. It has an f1 rating by Underwriters Laboratories Inc. Physical pr.. |
|||
Hot Ball Pressure Test | >= 125 °C | >= 257 °F | IEC 60335-1 |
Styron EMERGEâ„¢ 4850-19 Polycarbonate EMERGEâ„¢ 4850-19 advanced resin provides superior ignition resistance and ultraviolet light resistance in opaque applications. It has an f1 rating by Underwriters Laboratories Inc. Physical pr.. |
|||
Hot Ball Pressure Test | 125 °C | 257 °F | IEC 60695-10-2 |
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS Noryl NH6020 resin is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 .. |
|||
Hot Ball Pressure Test | 125 °C | 257 °F | IEC 60335-1 |
Styron CALIBREâ„¢ 302-6 Polycarbonate Resin Overview: CALIBREâ„¢ 300-6 Polycarbonate resins offer exceptional impact resistance, heat distortion resistance, and optical clarity as well as high melt strength for blow molding and sheet appli.. |
|||
Hot Ball Pressure Test | >= 125 °C | >= 257 °F | IEC 60335-1 |
Styron EMERGEâ„¢ 4800-19 Polycarbonate EMERGEâ„¢ 4800-19 advanced resin provides superior ignition resistance in opaque, injection molding applications. Physical properties and process-ability are outstanding for this class of polyca.. |
|||
Hot Ball Pressure Test | 125 °C @Thickness 2.00 mm |
257 °F @Thickness 0.0787 in |
EN 60695-10-2 |
Borealis Borcom™ WG140AI Polypropylene Borcom™ WG140AI is a polypropylene microcomposite intended for injection molding. This material has an excellent balance between impact strength and stiffness, high melt flow rate and gives a good.. |
|||
Hot Ball Pressure Test | <= 125 °C | <= 257 °F | IEC 60695-10-2 |
SABIC Innovative Plastics Lexan® SD9705 PC Copolymer (Europe-Africa-Middle East) High visocisty PC Copolymer, low smoke, flame retardant resinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |