Polymer Property : CTE, linear, Parallel to Flow = 112 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 112 µm/m-°C

@Temperature -40.0 - 40.0 °C
62.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP SP003 PA 12
LNP* LUBRICOMP* SP003 is a compound based on Nylon 12 resin containing 15% PTFE/Silicone. Added feature of this material is: Wear Resistant.
CTE, linear, Parallel to Flow 112 µm/m-°C

@Temperature -40.0 - 40.0 °C
62.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP SP003 PA 12 (Asia Pacific)
LNP* Lubricomp* SP003 is a compound based on Nylon 12 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.
CTE, linear, Parallel to Flow 112 µm/m-°C

@Temperature 25.6 - 149 °C
62.0 µin/in-°F

@Temperature 78.0 - 300 °F
Length
Saint-Gobain Rulon® 641 Grade Bearing/Seal PTFE
Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of..
CTE, linear, Parallel to Flow 112 µm/m-°C

@Temperature 25.6 - 93.3 °C
62.0 µin/in-°F

@Temperature 78.0 - 200 °F
Length
Saint-Gobain Rulon® LR Grade Bearing/Seal PTFE
Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of..
CTE, linear, Parallel to Flow 112 µm/m-°C

@Temperature 25.6 - 149 °C
62.0 µin/in-°F

@Temperature 78.0 - 300 °F
Length
Saint-Gobain Rulon® LR Grade Bearing/Seal PTFE
Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of..
CTE, linear, Parallel to Flow 112 µm/m-°C

@Temperature -40.0 - 40.0 °C
62.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP KF002L Acetal Homopoly
LNP* THERMOCOMP* KF002L is a compound based on Acetal Homopolymer resin containing 10% Glass Fiber. Added features of this material include: Low Extractible.
CTE, linear, Parallel to Flow 112 µm/m-°C

@Temperature -40.0 - 40.0 °C
62.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP KF002L Acetal Homopoly (Asia Pacific)
LNP* Thermocomp* KF002L is a compound based on Acetal Homopolymer resin containing Glass Fiber. Added features of this material include: Low Extractible.