Material Notes:
Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of friction, and excellent abrasion and corrosion resistance while running without lubrication. They are used in bearing and seal applications from temperature extremes of 400°F to over 500°F with and without additional lubricants. A unique property of Rulon® is the absence of stick slip, that is, erratic low-speed motion. PTFE = polytetrafluoroethyleneLR Grade Bearing/Seal PTFE: The best known, most widely used Rulon formulation. Rulon LR has a long reputation for high wear resistance, low friction, good electrical properties and chemical inertness. Not only does it make a great sleeve, flange or thrust bearing, but it can also be bonded to nearly any surface to provide wear resistance and reduce friction. Maroon in color.Suitable for use in environments of steam, wet, dry, vacuum. Mating surface of steel/stainless steel Rc 35 and higher. Material has electrical and thermal insulation properties.Markets for these products include Agricultural, Appliances, Automotive, Document Processing Equipment, Industrial, TransportationInformation provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Density 2.25 g/cc
0.0813 lb/in³
ASTM D792
Water Absorption 0.00 %

@Time 86400 sec
0.00 %

@Time 24.0 hour
Immersion
Water Absorption at Saturation 0.00 %
0.00 %
Mechanical Properties Metric English Comments
Hardness, Shore D 75
75
Tensile Strength 10.3 MPa
1490 psi
ASTM D638
Elongation at Break 150 %
150 %
ASTM D638
Compressive Yield Strength 6.89 MPa
1000 psi
Max load under tribological use
Izod Impact, Notched 3.20 J/cm
6.00 ft-lb/in
Coefficient of Friction, Dynamic 0.15 - 0.25
0.15 - 0.25
Dry vs. Steel
Coefficient of Friction, Static 0.15 - 0.25
0.15 - 0.25
Dry vs. Steel
Limiting Pressure Velocity 0.350 MPa-m/sec
10000 psi-ft/min
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 112 µm/m-°C

@Temperature 25.6 - 93.3 °C
62.0 µin/in-°F

@Temperature 78.0 - 200 °F
Length
112 µm/m-°C

@Temperature 25.6 - 149 °C
62.0 µin/in-°F

@Temperature 78.0 - 300 °F
Length
CTE, linear, Transverse to Flow 63.0 µm/m-°C

@Temperature 25.6 - 93.3 °C
35.0 µin/in-°F

@Temperature 78.0 - 200 °F
Diameter
63.0 µm/m-°C

@Temperature 25.6 - 149 °C
35.0 µin/in-°F

@Temperature 78.0 - 300 °F
Diameter
Thermal Conductivity 0.331 W/m-K
2.30 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 288 °C
550 °F
Minimum Service Temperature, Air -240 °C
-400 °F
Descriptive Properties Value Comments
Color Maroon
Users viewing this material also viewed the following: