Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 18.0 µm/m-°C @Temperature >=143 °C |
10.0 µin/in-°F @Temperature >=289 °F |
Above Tg; ISO 11359 |
Victrex® PEEK 450GL30 30% Glass Fiber Reinforced Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, F.. |
|||
CTE, linear, Parallel to Flow | 18.0 µm/m-°C @Temperature -40.0 - 150 °C |
10.0 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2310EPR PEI 30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
CTE, linear, Parallel to Flow | 18.0 µm/m-°C @Temperature 23.0 - 150 °C |
10.0 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 2310EPR PEI 30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
CTE, linear, Parallel to Flow | 18.0 µm/m-°C @Temperature -40.0 - 150 °C |
10.0 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2310EPR PEI (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
CTE, linear, Parallel to Flow | 18.0 µm/m-°C @Temperature 23.0 - 150 °C |
10.0 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 2310EPR PEI (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
CTE, linear, Parallel to Flow | 18.0 µm/m-°C @Temperature -40.0 - 150 °C |
10.0 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2310EPR PEI (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. Resin is RoHS compliant. UL94 V0 listing. |
|||
CTE, linear, Parallel to Flow | 18.0 µm/m-°C @Temperature 23.0 - 150 °C |
10.0 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 2310EPR PEI (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. Resin is RoHS compliant. UL94 V0 listing. |
|||
CTE, linear, Parallel to Flow | 18.0 µm/m-°C @Temperature 23.0 - 150 °C |
10.0 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 18.0 µm/m-°C @Temperature -40.0 - 150 °C |
10.0 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Parallel to Flow | 18.0 µm/m-°C @Temperature 23.0 - 150 °C |
10.0 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Parallel to Flow | 18.0 µm/m-°C @Temperature 23.0 - 150 °C |
10.0 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM SF2250 PEI Blend (Asia Pacific) High flow Ultem for thin wall application |
|||
CTE, linear, Parallel to Flow | 18.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
10.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Stat-kon DE002P PC LNP STAT-KON* DE002P is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the .. |
|||
CTE, linear, Parallel to Flow | 18.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
10.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Stat-kon DE002P PC LNP STAT-KON* DE002P is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the .. |
|||
CTE, linear, Parallel to Flow | 18.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
10.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON DEL33EC PC LNP STAT-KON* DEL33EC is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 15% PTFE. Added features include: Clean Compounding System, Electrically Conductive, Wear Resistant, Ea.. |
|||
CTE, linear, Parallel to Flow | 18.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
10.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON DEL33EC PC LNP STAT-KON* DEL33EC is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 15% PTFE. Added features include: Clean Compounding System, Electrically Conductive, Wear Resistant, Ea.. |
|||
CTE, linear, Parallel to Flow | 18.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
10.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON DEL33EC PC (Asia Pacific) LNP STAT-KON* DEL33EC is a compound based on Polycarbonate resin containing Carbon Fiber, PTFE. Added features of this material include: Clean Compounding System. |
|||
CTE, linear, Parallel to Flow | 18.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
10.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON DEL33EC PC (Asia Pacific) LNP STAT-KON* DEL33EC is a compound based on Polycarbonate resin containing Carbon Fiber, PTFE. Added features of this material include: Clean Compounding System. |
|||
CTE, linear, Parallel to Flow | 18.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
10.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Thermocomp LC006E PEEK LNP THERMOCOMP* LC006E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Am.. |
|||
CTE, linear, Parallel to Flow | 18.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
10.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp LC006E PEEK LNP THERMOCOMP* LC006E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Am.. |
|||
CTE, linear, Parallel to Flow | 18.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
10.0 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK2000 PC+ABS LNP* Thermocomp* Lexan_JK2000 compound is a 22% GR, ECO-compliant FR, PC+ABS for thinwall molding applications. |
|||
CTE, linear, Parallel to Flow | 18.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
10.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP LF006 PEEK (Asia Pacific) LNP* Thermocomp* LF006 is a compound based on Polyetheretherketone resin containing Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 18.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
10.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP UC006H PPA LNP THERMOCOMP* UC006H is a compound based on Polyphthalamide resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare. |
|||
CTE, linear, Parallel to Flow | 18.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
10.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Stat-kon DE002P PC (Asia Pacific) LNP STAT-KON* DE002P is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the .. |
|||
CTE, linear, Parallel to Flow | 18.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
10.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Stat-kon DE002P PC (Asia Pacific) LNP STAT-KON* DE002P is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the .. |
|||
CTE, linear, Parallel to Flow | 18.0 µm/m-°C @Temperature -40.0 - 150 °C |
10.0 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
CTE, linear, Parallel to Flow | 18.0 µm/m-°C @Temperature 23.0 - 150 °C |
10.0 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
CTE, linear, Parallel to Flow | 18.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
10.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON EX99550C PEI LNP* STAT-KON* EX99550C is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 18.0 µm/m-°C @Temperature 23.0 - 150 °C |
10.0 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM SF2250 PEI Blend High flow Ultem for thin wall application |
|||
CTE, linear, Parallel to Flow | 18.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
10.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON QEL329 PA 6/10 LNP STAT-KON* QEL329 is a compound based on Nylon 6/10 resin containing 10% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant, Flame Retardant.. |
|||
CTE, linear, Parallel to Flow | 18.0 µm/m-°C @Temperature <=143 °C |
10.0 µin/in-°F @Temperature <=289 °F |
Below Tg; ASTM D696 |
Victrex® PEEK 650GL30 30% Glass Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, color natural/beige.Typical.. |