Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 84.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics GELOY CR8510 ASA
ASA with outstanding UV exposure performance for both exterior and interior applications. F1 Rated.
CTE, linear, Parallel to Flow 84.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics GELOY CR8510 ASA
ASA with outstanding UV exposure performance for both exterior and interior applications. F1 Rated.
CTE, linear, Parallel to Flow 84.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics GELOY CR8510 ASA (Asia Pacific)
ASA with outstanding UV exposure performance for both exterior and interior applications. F1 Rated.
CTE, linear, Parallel to Flow 84.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics GELOY CR8510 ASA (Asia Pacific)
ASA with outstanding UV exposure performance for both exterior and interior applications. F1 Rated.
CTE, linear, Parallel to Flow 84.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Geloy FXTW26SK ASA
Next generation Geloy XTW ASA for high heat exterior applications. Outstanding weatherability and toughness. Metallic sparkle VisualFx.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 84.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Geloy XTWM206 ASA
Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 84.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Geloy XTWM206 ASA (Asia Pacific)
Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Asia Pacific regio..
CTE, linear, Parallel to Flow 84.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Geloy XTWM206 ASA (Europe-Africa-Middle East)
Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Europe-Africa-Midd..
CTE, linear, Parallel to Flow 84.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics GELOY CR7500 ASA (Europe-Africa-Middle East)
High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only.
CTE, linear, Parallel to Flow 84.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics GELOY CR7500 ASA (Europe-Africa-Middle East)
High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only.
CTE, linear, Parallel to Flow 84.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Geloy FXTW26SK ASA (Asia Pacific)
Next generation Geloy XTW ASA for high heat exterior applications. Outstanding weatherability and toughness. Metallic sparkle VisualFx.This data was supplied by SABIC-IP for the Asia Pacific region...
CTE, linear, Parallel to Flow 84.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Geloy FXTW26SK ASA (Europe-Africa-Middle East)
Next generation Geloy XTW ASA for high heat exterior applications. Outstanding weatherability and toughness. Metallic sparkle VisualFx.This data was supplied by SABIC-IP for the Europe-Africa-Middle..
CTE, linear, Parallel to Flow 84.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL WCV072 PPE+PP (Asia Pacific)
Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De..
CTE, linear, Parallel to Flow 84.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL WCV072 PPE+PP (Europe-Africa-Middle East)
Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De..
CTE, linear, Parallel to Flow 84.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP QAP22S PA 6/10 (Asia Pacific)
LNP* Lubricomp* QAP22S is a compound based on Nylon 6/10 resin containing PTFE, Aramid Fiber, Silicone. Added features of this material include: Internally Lubricated, Heat Stabilized.
CTE, linear, Parallel to Flow 84.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP QAP22S PA6.10
LNP* LUBRICOMP* QAP22S is a compound based on Nylon 6/10 resin containing 10% PTFE/Silicone, 10% Aramid Fiber. Added features of this material include: Wear Resistant, Heat Stabilized.
CTE, linear, Parallel to Flow 84.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® V2000DM PBT (Asia Pacific)
Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics.
CTE, linear, Parallel to Flow 84.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® V2000DM PBT (Asia Pacific)
Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics.
CTE, linear, Parallel to Flow 84.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® V2000DM PBT (Europe-Africa-Middle East)
Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics.
CTE, linear, Parallel to Flow 84.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® V2000DM PBT (Europe-Africa-Middle East)
Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics.
CTE, linear, Parallel to Flow 84.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp MX88073 PP (Asia Pacific)
LNP* Thermocomp* MX88073 is a compound based on Polypropylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Parallel to Flow 84.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL WCV072 PPE+PP
Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De..
CTE, linear, Parallel to Flow 84.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® V2000DM PBT
Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics.
CTE, linear, Parallel to Flow 84.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® V2000DM PBT
Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics.
CTE, linear, Parallel to Flow 84.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp MX88073 PP
LNP* Thermocomp* MX88073 is a compound based on Polypropylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 84.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics GELOY CR7500 ASA (Asia Pacific)
High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only.
CTE, linear, Parallel to Flow 84.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics GELOY CR7500 ASA (Asia Pacific)
High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only.
CTE, linear, Parallel to Flow 84.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics GELOY CR7500 ASA
High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only.
CTE, linear, Parallel to Flow 84.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics GELOY CR7500 ASA
High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only.