Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 47.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
26.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL4019 PC Lexan* EXL4019 is an opaque 9% Glass Fiber (GF) reinforced polycarbonate (PC) siloxane copolymer resin for injection molding (IM) applications requiring improved stiffness. This resin also offers im.. |
|||
CTE, linear, Parallel to Flow | 47.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
26.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL4019 PC Lexan* EXL4019 is an opaque 9% Glass Fiber (GF) reinforced polycarbonate (PC) siloxane copolymer resin for injection molding (IM) applications requiring improved stiffness. This resin also offers im.. |
|||
CTE, linear, Parallel to Flow | 47.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
26.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL4019 PC (Asia Pacific) Lexan* EXL4019 is an opaque 9% Glass Fiber (GF) reinforced polycarbonate (PC) siloxane copolymer resin for injection molding (IM) applications requiring improved stiffness. This resin also offers im.. |
|||
CTE, linear, Parallel to Flow | 47.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
26.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL4019 PC (Asia Pacific) Lexan* EXL4019 is an opaque 9% Glass Fiber (GF) reinforced polycarbonate (PC) siloxane copolymer resin for injection molding (IM) applications requiring improved stiffness. This resin also offers im.. |
|||
CTE, linear, Parallel to Flow | 47.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
26.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL4019 PC (Europe-Africa-Middle East) Lexan* EXL4019 is an opaque 9% Glass Fiber (GF) reinforced polycarbonate (PC) siloxane copolymer resin for injection molding (IM) applications requiring improved stiffness. This resin also offers im.. |
|||
CTE, linear, Parallel to Flow | 47.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
26.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL4019 PC (Europe-Africa-Middle East) Lexan* EXL4019 is an opaque 9% Glass Fiber (GF) reinforced polycarbonate (PC) siloxane copolymer resin for injection molding (IM) applications requiring improved stiffness. This resin also offers im.. |
|||
CTE, linear, Parallel to Flow | 47.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
26.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL5689 PC Copolymer (Asia Pacific) Lexan* EXL5689 polycarbonate (PC) resin is a GF reinforced, UV stabilized, flame retardant injection molding copolymer blend. This medium flow resin features UL94 V0 @ 1.5mm flame retardancy based .. |
|||
CTE, linear, Parallel to Flow | 47.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
26.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL5689 PC Copolymer (Asia Pacific) Lexan* EXL5689 polycarbonate (PC) resin is a GF reinforced, UV stabilized, flame retardant injection molding copolymer blend. This medium flow resin features UL94 V0 @ 1.5mm flame retardancy based .. |
|||
CTE, linear, Parallel to Flow | 47.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
26.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL5689 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL5689 polycarbonate (PC) resin is a GF reinforced, UV stabilized, flame retardant injection molding copolymer blend. This medium flow resin features UL94 V0 @ 1.5mm flame retardancy based .. |
|||
CTE, linear, Parallel to Flow | 47.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
26.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL5689 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL5689 polycarbonate (PC) resin is a GF reinforced, UV stabilized, flame retardant injection molding copolymer blend. This medium flow resin features UL94 V0 @ 1.5mm flame retardancy based .. |
|||
CTE, linear, Parallel to Flow | 47.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
26.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.. |
|||
CTE, linear, Parallel to Flow | 47.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
26.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.. |
|||
CTE, linear, Parallel to Flow | 47.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
26.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer (Asia Pacific) Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.. |
|||
CTE, linear, Parallel to Flow | 47.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
26.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer (Asia Pacific) Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.. |
|||
CTE, linear, Parallel to Flow | 47.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
26.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer (Europe-Africa-Middle East) Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.. |
|||
CTE, linear, Parallel to Flow | 47.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
26.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer (Europe-Africa-Middle East) Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.. |
|||
CTE, linear, Parallel to Flow | 47.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
26.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36ELH PC LNP* Lubricomp* DFL36ELH is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractible, Easy Moldi.. |
|||
CTE, linear, Parallel to Flow | 47.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
26.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36XXJ PC LNP* Lubricomp* DFL36XXJ is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractable, Healthcare.. |
|||
CTE, linear, Parallel to Flow | 47.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
26.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DFL23 PC LNP* Lubricomp* DFL23 is a compound based on Polycarbonate resin containing 15% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 47.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
26.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36ELH PC (Asia Pacific) LNP* Lubricomp* DFL36ELH is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
CTE, linear, Parallel to Flow | 47.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
26.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP ZFG26 PPE+PS LNP* LUBRICOMP* ZFG26 is a compound based on PPE+PS resin containing 30% Glass Fiber, 10% Graphite. Added features of this material include: Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 47.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
26.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP ZFG26 PPE+PS (Asia Pacific) LNP* Lubricomp* ZFG26 is a compound based on PPE+PS Blend resin containing Glass Fiber, Graphite Powder. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 47.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
26.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON ZE0039 MODIFIED POLYPHENYLENE (Asia Pacific) LNP* Stat-kon* ZE0039 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber. |
|||
CTE, linear, Parallel to Flow | 47.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
26.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Stat-kon ZE0039 MODIFIED POYPHENYLENE LNP* Stat-kon* ZE0039 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 47.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
26.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Stat-kon ZE0039 MODIFIED POYPHENYLENE (Asia Pacific) LNP* Stat-kon* ZE0039 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Parallel to Flow | 47.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
26.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON ZE0039 PPO LNP* STAT-KON* ZE0039 is a compound based on PPO resin containing 15% Carbon Fiber. Added features of this grade includes: Flame Retardant, Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 47.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
26.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL5689 PC Copolymer Lexan* EXL5689 polycarbonate (PC) resin is a GF reinforced, UV stabilized, flame retardant injection molding copolymer blend. This medium flow resin features UL94 V0 @ 1.5mm flame retardancy based .. |
|||
CTE, linear, Parallel to Flow | 47.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
26.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL5689 PC Copolymer Lexan* EXL5689 polycarbonate (PC) resin is a GF reinforced, UV stabilized, flame retardant injection molding copolymer blend. This medium flow resin features UL94 V0 @ 1.5mm flame retardancy based .. |
|||
CTE, linear, Parallel to Flow | 47.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
26.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DFP34 PC (Asia Pacific) LNP* Lubricomp* DFP34 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 47.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
26.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DFP34 PC LNP* Lubricomp* DFP34 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Internally Lubricated. |