Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 23.0 - 55.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Crastin® S600F20 NC010 PBT
(Unverified Data**) Crastin® S600F20 NC010 is an unreinforced, lubricated, medium viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 100 - 200 °C |
66.7 µin/in-°F @Temperature 212 - 392 °F |
ASTM E831 |
Solvay Specialty Polymers Amodel® AE-4133 Polyphthalamide (PPA)
(Unverified Data**) Amodel AE-4133 is a 33% glass reinforced, hot-water moldable polyphthalamide (PPA) designed to work in the modern automotive electrical environment. This grade features a high heat deflection temper.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 100 - 200 °C |
66.7 µin/in-°F @Temperature 212 - 392 °F |
ASTM E831 |
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 100 - 200 °C |
66.7 µin/in-°F @Temperature 212 - 392 °F |
ASTM E831 |
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin. Th.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 23.0 - 55.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 500AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 500AL is a medium viscosity acetal homopolymer, with an advanced system of lubrication for applications requiring low wear and/or coefficient of friction against steel, itself or other plas.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 23.0 - 55.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612
(Unverified Data**) Zytel® 151 NC010 is a PA 612 resin.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 23.0 - 55.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 131 °F |
|
Aardvark Polymers AARTEL® 2100UV Acetal Homopolymer Rotational Molding Resin Aartel 2100UV is a natural acetal homopolymer with UV stabilizers.Aartel 2100UV is a medium viscosity resin with excellent flow characteristics.Aartel 2100UV is available in natural white and may be.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature -30.0 - 80.0 °C |
66.7 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL ZX09022 PPE+PP (Europe-Africa-Middle East) Thermocomp ZX09022 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile mod.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 100 - 200 °C |
66.7 µin/in-°F @Temperature 212 - 392 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® A-4145 HH Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® A-4145 HH is a 45% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation .. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 100 - 200 °C |
66.7 µin/in-°F @Temperature 212 - 392 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Testing conducted on samp.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 100 - 200 °C |
66.7 µin/in-°F @Temperature 212 - 392 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA), 16% Glass Fiber (Dry) Amodel® AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 100 - 200 °C |
66.7 µin/in-°F @Temperature 212 - 392 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA), 15% Glass Fiber (Dry) Amodel® AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 150 - 200 °C |
66.7 µin/in-°F @Temperature 302 - 392 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Lavanta® 5115 WH224 Polyester, High Performance (HPP), 15% Glass Fiber Lavanta® 5115 WH224 is a 15% glass fiber reinforced, high-performance polyester (HPP) injection molding grade developed specifically for HB LED packaging applications that utilize surface mount t.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature -40.0 - 40.0 °C |
66.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® 420HP PBT 30% Glass filled PBT resin, FDA Food Contact compliant in limited colors. Effective March 2008 this grade will no longer be supported with biocompatibility information. Alternative grade Valox HX420.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature -30.0 - 80.0 °C |
66.7 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP ZX09022 PPE+PP (Europe-Africa-Middle East) Thermocomp ZX09022 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile mod.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature -40.0 - 40.0 °C |
66.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® V2105U PBT (Europe-Africa-Middle East) Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 23.0 - 60.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® VX4910 ASA+PBT (Europe-Africa-Middle East) 10% Glass reinforced nucleated PBT/ASA with excellent mechanical properties high dimensional stability, and low density. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature -30.0 - 80.0 °C |
66.7 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus .. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature -30.0 - 80.0 °C |
66.7 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP (Europe-Africa-Middle East) Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus .. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature -30.0 - 80.0 °C |
66.7 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL PPX ZX09022 PPE+PP (Europe-Africa-Middle East) Thermocomp ZX09022 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile mod.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature -50.0 - 50.0 °C |
66.7 µin/in-°F @Temperature -58.0 - 122 °F |
ISO 11359-2 |
Chevron Phillips Xtel® XE3035NA Polyphenylene Sulfide Alloy Xtel® XE3035NA is a high performance, glass fiber reinforced, PPS based alloy developed to provide exceptionally high ductility and impact resistance along with good thermal stability.Information p.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 23.0 - 55.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® ST801AHS NC010 Nylon 66
(Unverified Data**) Zytel® ST801AHS NC010 is a Super Tough, high performance polyamide 66 resin. It offers outstanding molding performance in injection molding applications.Information provided by DuPont |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 23.0 - 55.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ASTM E 831 |
DuPont Performance Polymers Zytel® ST801AHS NC010 Nylon 66
(Unverified Data**) Zytel® ST801AHS NC010 is a Super Tough, high performance polyamide 66 resin. It offers outstanding molding performance in injection molding applications.Information provided by DuPont |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 55.0 - 160 °C |
66.7 µin/in-°F @Temperature 131 - 320 °F |
DAM; ASTM E 831 |
DuPont Performance Polymers Zytel® ST801AW NC010 Nylon 66
(Unverified Data**) Zytel® ST801AW NC010 is a Super Tough, high performance polyamide 66 resin. It is UV stabilized and when appropriately colored offers the best resistance to indirect sunlight in automotive interior.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 55.0 - 160 °C |
66.7 µin/in-°F @Temperature 131 - 320 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® ST801AW NC010 Nylon 66
(Unverified Data**) Zytel® ST801AW NC010 is a Super Tough, high performance polyamide 66 resin. It is UV stabilized and when appropriately colored offers the best resistance to indirect sunlight in automotive interior.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 149 - 249 °C |
66.7 µin/in-°F @Temperature 300 - 480 °F |
ASTM E831 |
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications incl.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 149 - 249 °C |
66.7 µin/in-°F @Temperature 300 - 480 °F |
ASTM E831 |
Solvay Specialty Polymers Amodel® AS-4133 HN Polyphthalamide (PPA), Dry, 33% Glass Fiber Reinforcement, Heat Stabilizer Amodel AS-4133 HN polyphthalamide (PPA) is a non-lubricated, heat stabilized grade that offers fast cycle times and is hot-water moldable. Typical applications include electrical and electronic comp.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature -40.0 - 40.0 °C |
66.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® V2105U PBT (Asia Pacific) Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 55.0 - 160 °C |
66.7 µin/in-°F @Temperature 131 - 320 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness and sur.. |
|||
CTE, linear, Transverse to Flow | 120 µm/m-°C @Temperature 23.0 - 55.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® SC315 NC010 Nylon 612