Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 25.0 µm/m-°C

@Temperature -100 °C
13.9 µin/in-°F

@Temperature -148 °F
Chevron Phillips Ryton® A-200 PPS Polyphenylene Sulfide  (discontinued **)
Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol..
CTE, linear, Transverse to Flow 25.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
13.9 µin/in-°F

@Temperature -58.0 - 122 °F
ISO 11359-2
Solvay Specialty Polymers Ryton® R-7-190BL Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® R-7-190BL glass fiber and mineral filled polyphenylene sulfide compound provides enhanced strength and low maintenance molding using conventional molding equipment.Features: Good Chemical ..
CTE, linear, Transverse to Flow 25.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
13.9 µin/in-°F

@Temperature -58.0 - 122 °F
ISO 11359-2
Solvay Specialty Polymers Ryton® R-7-190NA Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® R-7-190NA glass fiber and mineral filled polyphenylene sulfide compound provides enhanced strength and low maintenance molding using conventional molding equipment.Features: Good Chemical ..
CTE, linear, Transverse to Flow 25.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
13.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP GF004 PSU
LNP* Thermocomp* GF004 is a compound based on Polysulfone resin containing 20% Glass Fiber.
CTE, linear, Transverse to Flow 25.0 µm/m-°C

@Temperature <=250 °C
13.9 µin/in-°F

@Temperature <=482 °F
z (< Tg); IPC TM-650 2.4.24
Arlon EP2 Enhanced Polyimide Laminate and Prepreg
High reliability and high temperature materialEP2 Enhanced Polyimide is the next generation of polyimide and prepreg products, engineered for improved properties and processing and for applications ..
CTE, linear, Transverse to Flow 25.0 µm/m-°C

@Thickness 4.00 mm,
Temperature 175 °C
13.9 µin/in-°F

@Thickness 0.157 in,
Temperature 347 °F
BASF Ultrason® KR 4113 PESU with 10/10% Carbon Fibers/Graphite and 10% PTFE
Description: Compound based on PES with 30 % filler. The filler system, a mixture of carbon fibers, graphite and PTFE powder, considerably improves Ultrason’s tribological properties. In addition, ..
CTE, linear, Transverse to Flow 25.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
13.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP GF004 PSU (Asia Pacific)
LNP* Thermocomp* GF004 is a compound based on Polysulfone resin containing Glass Fiber.