Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 30.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
16.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP KONDUIT OX11314 PPS (Europe-Africa-Middle East) Thermally conductive mineral and glass fiber filled PPS Eco-FR compound |
|||
CTE, linear, Transverse to Flow | 30.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
16.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36ELH PC LNP* Lubricomp* DFL36ELH is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractible, Easy Moldi.. |
|||
CTE, linear, Transverse to Flow | 30.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
16.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36ELH PC (Asia Pacific) LNP* Lubricomp* DFL36ELH is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
CTE, linear, Transverse to Flow | 30.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
16.7 µin/in-°F @Temperature -58.0 - 122 °F |
ISO 11359-2 |
Chevron Phillips Ryton® R-7-220NA Polyphenylene Sulfide Resin
(discontinued **) Ryton® R-7-220 is a glass and mineral filled polyphenylene sulfide compound developed to provide good mechanical strength and enhanced hydrolytic stability in applications requiring constant or rep.. |
|||
CTE, linear, Transverse to Flow | 30.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
16.7 µin/in-°F @Temperature -58.0 - 122 °F |
ISO 11359-2 |
Solvay Specialty Polymers Ryton® R-7-220BL Polyphenylene Sulfide Resin
(Unverified Data**) Ryton® R-7-220 is a glass and mineral filled polyphenylene sulfide compound developed to provide good mechanical strength and enhanced hydrolytic stability in applications requiring constant or rep.. |
|||
CTE, linear, Transverse to Flow | 30.0 µm/m-°C @Temperature -40.0 - 150 °C |
16.7 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2310EPR PEI 30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
CTE, linear, Transverse to Flow | 30.0 µm/m-°C @Temperature 23.0 - 150 °C |
16.7 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 2310EPR PEI 30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
CTE, linear, Transverse to Flow | 30.0 µm/m-°C @Temperature -40.0 - 150 °C |
16.7 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2310EPR PEI (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
CTE, linear, Transverse to Flow | 30.0 µm/m-°C @Temperature 23.0 - 150 °C |
16.7 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 2310EPR PEI (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
CTE, linear, Transverse to Flow | 30.0 µm/m-°C @Temperature -40.0 - 150 °C |
16.7 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2310EPR PEI (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. Resin is RoHS compliant. UL94 V0 listing. |
|||
CTE, linear, Transverse to Flow | 30.0 µm/m-°C @Temperature 23.0 - 150 °C |
16.7 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 2310EPR PEI (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. Resin is RoHS compliant. UL94 V0 listing. |
|||
CTE, linear, Transverse to Flow | 30.0 µm/m-°C @Temperature 23.0 - 150 °C |
16.7 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem 2412EPR PEI 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Am.. |
|||
CTE, linear, Transverse to Flow | 30.0 µm/m-°C @Temperature -40.0 - 150 °C |
16.7 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem 2412EPR PEI (Asia Pacific) 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the As.. |
|||
CTE, linear, Transverse to Flow | 30.0 µm/m-°C @Temperature -40.0 - 150 °C |
16.7 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem 2412EPR PEI (Europe-Africa-Middle East) 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu.. |
|||
CTE, linear, Transverse to Flow | 30.0 µm/m-°C @Temperature 23.0 - 150 °C |
16.7 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem 2412EPR PEI (Europe-Africa-Middle East) 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu.. |
|||
CTE, linear, Transverse to Flow | 30.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
16.7 µin/in-°F @Temperature -58.0 - 122 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Ryton® BR111 Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® BR111 is a natural-colored glass fiber and mineral filled polyphenylene sulfide compound that provides enhanced mechanical strength with good electrical properties and outstanding chemical.. |
|||
CTE, linear, Transverse to Flow | 30.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
16.7 µin/in-°F @Temperature -58.0 - 122 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Ryton® BR111BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® BR111BL Ryton® BR111 is a black-colored glass fiber and mineral filled polyphenylene sulfide compound that provides enhanced mechanical strength with good electrical properties and outs.. |
|||
CTE, linear, Transverse to Flow | 30.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
16.7 µin/in-°F @Temperature -58.0 - 122 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Ryton® R-7-120BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-120NA and R-7-120BL glass fiber and mineral filled polyphenylene sulfide compounds provide good strength and low maintenance molding using conventional molding equipment.Features: Good.. |
|||
CTE, linear, Transverse to Flow | 30.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
16.7 µin/in-°F @Temperature -58.0 - 122 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Ryton® R-7-120NA Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-120NA and R-7-120BL glass fiber and mineral filled polyphenylene sulfide compounds provide good strength and low maintenance molding using conventional molding equipment.Features: Good.. |
|||
CTE, linear, Transverse to Flow | 30.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
16.7 µin/in-°F @Temperature -58.0 - 122 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Ryton® R-7-121BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-121NA and R-7-121BL glass fiber and mineral filled polyphenylene sulfide compounds provide good mechanical strength with good flow and low maintenance molding using conventional moldin.. |
|||
CTE, linear, Transverse to Flow | 30.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
16.7 µin/in-°F @Temperature -58.0 - 122 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Ryton® R-7-121NA Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-121NA and R-7-121BL glass fiber and mineral filled polyphenylene sulfide compounds provide good mechanical strength with good flow and low maintenance molding using conventional moldin.. |
|||
CTE, linear, Transverse to Flow | 30.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
16.7 µin/in-°F @Temperature -58.0 - 122 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Ryton® R-7-220BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-220BL glass fiber and mineral filled polyphenylene sulfide compound provides enhanced mechanical strength after constant or repeated exposure to high temperature water.Features: Good S.. |
|||
CTE, linear, Transverse to Flow | 30.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
16.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® SHF436HR PBT PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant. |
|||
CTE, linear, Transverse to Flow | 30.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
16.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® SHF436HR PBT PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant. |
|||
CTE, linear, Transverse to Flow | 30.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
16.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® SHF436HR PBT (Asia Pacific) PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant. |
|||
CTE, linear, Transverse to Flow | 30.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
16.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® SHF436HR PBT (Asia Pacific) PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant. |
|||
CTE, linear, Transverse to Flow | 30.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
16.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® SHF436HR PBT (Europe-Africa-Middle East) PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant. |
|||
CTE, linear, Transverse to Flow | 30.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
16.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® SHF436HR PBT (Europe-Africa-Middle East) PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant. |
|||
CTE, linear, Transverse to Flow | 30.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
16.7 µin/in-°F @Temperature -58.0 - 122 °F |
ISO 11359-2 |
Solvay Specialty Polymers Ryton® R-7-121NA Polyphenylene Sulfide Resin
(Unverified Data**) Ryton® R-7-121NA is an advanced glass/mineral filled polyphenylene sulfide compound developed to provide good mechanical strength with good flow and low maintenance molding using conventional moldi.. |
|||
CTE, linear, Transverse to Flow | 30.0 µm/m-°C @Temperature -100 °C |
16.7 µin/in-°F @Temperature -148 °F |
|
Chevron Phillips Ryton® R-4 04 PPS (Polyphenylene Sulfide)
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |