Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 62.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 9931X PC (Europe-Africa-Middle East) Lexan* 9931X is a UV stabilized high flow opaque injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, extreme low temperatu.. |
|||
CTE, linear, Transverse to Flow | 62.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® 9931X PC (Europe-Africa-Middle East) Lexan* 9931X is a UV stabilized high flow opaque injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, extreme low temperatu.. |
|||
CTE, linear, Transverse to Flow | 62.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL9134 PC Copolymer Lexan* EXL9134 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high flow opaque injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, .. |
|||
CTE, linear, Transverse to Flow | 62.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL9134 PC Copolymer Lexan* EXL9134 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high flow opaque injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, .. |
|||
CTE, linear, Transverse to Flow | 62.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® SLX1432 PC Copolymer Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in opaque colors. Typical minimum color tolerance limit is DE CMC < 1.0 |
|||
CTE, linear, Transverse to Flow | 62.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® SLX1432 PC Copolymer Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in opaque colors. Typical minimum color tolerance limit is DE CMC < 1.0 |
|||
CTE, linear, Transverse to Flow | 62.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics GELOY XTPMFR10 ASA+PC (Asia Pacific) Improved ASA/PC blend for high flow, 1.0mm V0 applications. Improved UV performance aesthetically and physically compared to alternatives. |
|||
CTE, linear, Transverse to Flow | 62.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL9134 PC Copolymer (Asia Pacific) Lexan* EXL9134 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high flow opaque injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, .. |
|||
CTE, linear, Transverse to Flow | 62.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL9134 PC Copolymer (Asia Pacific) Lexan* EXL9134 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high flow opaque injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, .. |
|||
CTE, linear, Transverse to Flow | 62.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL9134 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL9134 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high flow opaque injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, .. |
|||
CTE, linear, Transverse to Flow | 62.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL9134 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL9134 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high flow opaque injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, .. |
|||
CTE, linear, Transverse to Flow | 62.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® SLX1432 PC Copolymer (Asia Pacific) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in opaque colors. Typical minimum color tolerance limit is DE CMC < 1.0 |
|||
CTE, linear, Transverse to Flow | 62.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® SLX1432 PC Copolymer (Asia Pacific) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in opaque colors. Typical minimum color tolerance limit is DE CMC < 1.0 |
|||
CTE, linear, Transverse to Flow | 62.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® SLX1432 PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in opaque colors. Typical minimum color tolerance limit is DE CMC < 1.0 |
|||
CTE, linear, Transverse to Flow | 62.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® SLX1432 PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in opaque colors. Typical minimum color tolerance limit is DE CMC < 1.0 |
|||
CTE, linear, Transverse to Flow | 62.0 µm/m-°C @Temperature 23.0 - 150 °C |
34.4 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM SF2360 PEI Blend (Asia Pacific) High flow Ultem for thin wall application |
|||
CTE, linear, Transverse to Flow | 62.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® EH7020HF PBT+PET (Asia Pacific) Valox EH7020HF is a mineral filled PBT/PET that offers good surface appearance, high flow and good heat performance. EH7020HF was developped for automotiove bezel application that require basecoat +.. |
|||
CTE, linear, Transverse to Flow | 62.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® EH7020HF PBT+PET (Asia Pacific) Valox EH7020HF is a mineral filled PBT/PET that offers good surface appearance, high flow and good heat performance. EH7020HF was developped for automotiove bezel application that require basecoat +.. |
|||
CTE, linear, Transverse to Flow | 62.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® EH7025AG PBT+PET Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application. |
|||
CTE, linear, Transverse to Flow | 62.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® EH7025AG PBT+PET (Asia Pacific) Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application. |
|||
CTE, linear, Transverse to Flow | 62.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® EH7025AG PBT+PET (Europe-Africa-Middle East) Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application. |
|||
CTE, linear, Transverse to Flow | 62.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® ENH4560 PBT (Europe-Africa-Middle East) Valox* ENH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* PBT resin. |
|||
CTE, linear, Transverse to Flow | 62.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-LOY AF3009 ABS LNP* STAT-LOY* AF3009 is a compound based on ABS resin containing 10% Glass Fiber. Added features of this material include: Antistatic, Flame Retardant. |
|||
CTE, linear, Transverse to Flow | 62.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-LOY AF3009 ABS (Asia Pacific) LNP* Stat-loy* AF3009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, Flame Retardant. Added features of this material include: Antistat, Flame Retardant. |
|||
CTE, linear, Transverse to Flow | 62.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
34.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-LOY AF3009 ABS (Asia Pacific) LNP* Stat-loy* AF3009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, Flame Retardant. Added features of this material include: Antistat, Flame Retardant. |
|||
CTE, linear, Transverse to Flow | 62.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
34.4 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® HTN FR52G30NHF BK337 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFR52G30NHF BK337 is a 30% glass reinforced, flame retardant, lubricated high performance polyamide resin with improved flow. It is also a PPA resin and it uses a non-halogenated flame ret.. |