Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat Distortion Temperature | 240 °C | 464 °F | ISO 75-2 |
Tisan TISLAMID® 66 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Heat Distortion Temperature | 240 °C | 464 °F | ISO 75-2 |
Tisan TISLAMID® 66 30% Glass Bead Reinforced Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Heat Distortion Temperature | 240 °C | 464 °F | ISO 75-2 |
Tisan TISLAMID® 66 30% Glass Filled Impact Modified, Heat Stabilized Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |