Thermal Properties Metric English Comments
Specific Heat Capacity 1.39 J/g-°C

@Temperature 50.0 °C
0.332 BTU/lb-°F

@Temperature 122 °F
ASTM C351
Solvay Specialty Polymers AvaSpire® AV-630 Polyaryletherketone (PAEK)
AvaSpire® AV-630 is an unreinforced polyaryletherketone (PAEK) developed as an alternative to low melt flow PEEK for the extrusion of ultra-thin films. Films with thicknesses as low as 0.2 mils (..
Specific Heat Capacity 1.39 J/g-°C

@Pressure 20.3 MPa,
Temperature 24.0 °C
0.332 BTU/lb-°F

@Pressure 2940 psi,
Temperature 75.2 °F
3M Interam™ E-5A-4 Endothermic Mat
When properly installed, 3M Interam Endothermic Mat E-5A-4 provides a uniform covering that, when exposed to high temperatures, releases chemically-bound water to cool the outer surfaces of the wrap..
Specific Heat Capacity 1.39 J/g-°C

@Temperature 50.0 °C
0.332 BTU/lb-°F

@Temperature 122 °F
DSC
Solvay Specialty Polymers AvaSpire® AV-630 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-630 is an unreinforced polyaryletherketone (PAEK) developed as an alternative to low melt flow PEEK for the extrusion of ultra-thin films. Films with thicknesses as low as 0.2 mils (5 mi..