Processing Properties Metric English Comments
Processing Temperature 238 - 249 °C
460 - 480 °F
At Nozzle
Nylene® 451 Nylon 6
Dry as molded. Injection molding grade. Nylene 451 is recommended for molding applications requiring both maximum durability and toughness. Exceptional fatigue and wear resistance insure long produ..
Processing Temperature 238 - 249 °C
460 - 480 °F
At Nozzle
Nylene® 451 Nylon 6, 50% RH
Injection molding grade. Nylene 451 is recommended for molding applications requiring both maximum durability and toughness. Exceptional fatigue and wear resistance insure long product life to gears..
Processing Temperature 45.0 - 249 °C
113 - 480 °F
Average value: 171 °C Grade Count:5
Overview of materials for PETG Copolyester
This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M..
Processing Temperature 199 - 249 °C
390 - 480 °F
Total PPC M6823MZ Metallocene Isostatic Propylene Polymer
TOTAL Petrochemicals Polypropylene M6823MZ is an isostatic form of copolymer polypropylene made via TOTAL Petrochemicals proprietary metallocene catalyst technology.Clarity. M6823MZ incorporates th..
Processing Temperature 193 - 249 °C
380 - 480 °F
Average value: 222 °C Grade Count:9
Overview of materials for Acrylic/Polycarbonate Alloy
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy". Each property range of values reported is minimum and maximum values of ap..
Processing Temperature 202 - 249 °C
395 - 480 °F
Average value: 225 °C Grade Count:9
Overview of materials for Acrylic/Polycarbonate Alloy, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Glass Fiber Filler". Each property range of values reported is minimum and ..
Processing Temperature 202 - 249 °C
395 - 480 °F
Average value: 225 °C Grade Count:4
Overview of materials for Acrylic/Polycarbonate Alloy, Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Carbon Fiber Filler". Each property range of values reported is minimum and..