Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 82.2 - 93.3 °C | 180 - 200 °F | Prepolymer Temperature |
Northstar Polymers MGB-A80AQ High Performance Polyurethane Cast Elastomer System 80A This is a PTMEG/MDI base high-performance polyurethane casting system. This system is recommended to applications in which the part requires high rebound, slide abrasion, constant water contact and.. |
|||
Processing Temperature | 82.2 - 93.3 °C | 180 - 200 °F | Prepolymer Temperature |
Northstar Polymers MGB-A90A High Performance Polyurethane Cast Elastomer System 90A This is a PTMEG/MDI base high-performance polyurethane casting system. This system is recommended to applications in which the part requires high rebound, slide abrasion, constant water contact and.. |
|||
Processing Temperature | 82.2 - 93.3 °C | 180 - 200 °F | Prepolymer Temperature |
Northstar Polymers MSB-A95A High Performance Polyurethane Cast Elastomer System This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires high tensile strength, cut/tear resistance, dry-abrasio.. |
|||
Processing Temperature | 82.2 - 93.3 °C | 180 - 200 °F | Prepolymer Temperature |
Northstar Polymers MSS-A85C Ester Base Polyurethane This high performance polyester system is one of a family of polymer systems developed by Northstar Polymers for demanding work environments. Urethane elastomers molded with this system exhibit hig.. |
|||
Processing Temperature | 82.2 - 93.3 °C | 180 - 200 °F | Prepolymer Temperature |
Northstar Polymers MSS-A90A High Performance Polyurethane Cast Elastomer System 90A This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires high tensile strength, cut/tear resistance, dry-abrasio.. |
|||
Processing Temperature | 82.2 - 93.3 °C | 180 - 200 °F | Prepolymer Temperature |
Northstar Polymers MSS-A95BQ Ester Base High Performance Polyurethane This high-performance quasi-polyester system is one of a family of polymer systems developed by Northstar Polymers for demanding work environments. Urethane elastomers molded with this system exhib.. |
|||
Processing Temperature | 82.2 - 93.3 °C | 180 - 200 °F | Curing Agent Temperature |
Northstar Polymers MSS-A95BQ Ester Base High Performance Polyurethane This high-performance quasi-polyester system is one of a family of polymer systems developed by Northstar Polymers for demanding work environments. Urethane elastomers molded with this system exhib.. |
|||
Processing Temperature | 18.3 - 93.3 °C | 65.0 - 200 °F | Average value: 42.8 °C Grade Count:26 |
Overview of materials for Thermoset Polyurethane, Liquid This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Liquid". Each property range of values reported is minimum and maximum values of.. |
|||
Processing Temperature | 82.2 - 93.3 °C | 180 - 200 °F | Prepolymer Temperature |
Northstar Polymers MGG-A70DQ High Performance Polyurethane Cast Elastomer System 70A This is a PTMEG/MDI base high-performance polyurethane casting system. This system is recommended to applications in which the part requires high rebound, slide abrasion, constant water contact and.. |
|||
Processing Temperature | 82.2 - 93.3 °C | 180 - 200 °F | Prepolymer Temperature |
Northstar Polymers MGP-D50A High Performance Polyurethane Cast Elastomer System 50D This is a PTMEG/MDI base high-performance polyurethane casting system. This system is recommended to applications in which the part requires some load-bearing, slide abrasion, constant water contac.. |