Northstar Polymers MSS-A90A High Performance Polyurethane Cast Elastomer System 90A

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Liquid
Manufacturer Northstar Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Northstar Polymers MSS-A90A High Performance Polyurethane Cast Elastomer System 90A.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires high tensile strength, cut/tear resistance, dry-abrasion resistance, slow response speed, and low energy rebound/response. Ester base systems are generally less expensive than PTMEG base material. Possible applications for this material include skirting for conveyer belts, abrasion resistance liners and parts, and other specialty parts. This is a conventional “full-prepolymer” type material cured with 1,4 BDO. Can be approved for FDA dry food contact.Information provided by Northstar Polymers.
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
ASTM D2240
Tensile Strength 29.0 MPa
4200 psi
ASTM D412
Elongation at Break 650 %
650 %
ASTM D412
Rebound 28 %
28 %
Bashore Rebound; ASTM D2632
Tear Strength 52.6 kN/m
300 pli
Split; ASTM D624
105 kN/m
600 pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 62
62
ASTM D4060
Processing Properties Metric English Comments
Processing Temperature 25.0 °C
77.0 °F
Curing Agent Temperature
82.2 - 93.3 °C
180 - 200 °F
Prepolymer Temperature
Mold Temperature 82.2 - 93.3 °C
180 - 200 °F
Cure Time 30.0 min

@Temperature 93.3 °C
0.500 hour

@Temperature 200 °F
De-mold Time
960 min

@Temperature 82.2 °C
16.0 hour

@Temperature 180 °F
Complete Cure Cycle
Pot Life 2.50 - 3.00 min
2.50 - 3.00 min
Descriptive Properties Value Comments
Curing Agent BNA-005
Prepolymer MSA-052