Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 232 - 266 °C | 450 - 510 °F | Average value: 249 °C Grade Count:21 |
Overview of materials for Polycarbonate/ABS Alloy, NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, NCG Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Processing Temperature | 216 - 266 °C | 420 - 510 °F | Average value: 244 °C Grade Count:5 |
Overview of materials for Nylon 12, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Processing Temperature | 216 - 266 °C | 420 - 510 °F | Average value: 246 °C Grade Count:11 |
Overview of materials for Nylon 12, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Processing Temperature | 216 - 266 °C | 420 - 510 °F | Average value: 244 °C Grade Count:8 |
Overview of materials for Nylon 12, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Processing Temperature | 216 - 266 °C | 420 - 510 °F | Average value: 241 °C Grade Count:5 |
Overview of materials for Nylon 12, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Processing Temperature | 216 - 266 °C | 420 - 510 °F | Average value: 241 °C Grade Count:3 |
Overview of materials for Nylon 12, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |