Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, PTFE Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.03 - 1.14 g/cc
0.0372 - 0.0412 lb/in³
Average value: 1.10 g/cc Grade Count:10
Water Absorption 0.100 - 0.500 %
0.100 - 0.500 %
Average value: 0.229 % Grade Count:7
Linear Mold Shrinkage 0.00700 - 0.0200 cm/cm
0.00700 - 0.0200 in/in
Average value: 0.0142 cm/cm Grade Count:10
Mechanical Properties Metric English Comments
Hardness, Rockwell R 106 - 108
106 - 108
Average value: 107 Grade Count:3
Tensile Strength, Ultimate 31.0 - 50.0 MPa
4500 - 7250 psi
Average value: 40.8 MPa Grade Count:9
Elongation at Break 4.50 - 20.0 %
4.50 - 20.0 %
Average value: 10.6 % Grade Count:8
Modulus of Elasticity 1.24 - 2.30 GPa
180 - 334 ksi
Average value: 1.65 GPa Grade Count:8
Flexural Yield Strength 37.9 - 75.0 MPa
5500 - 10900 psi
Average value: 56.4 MPa Grade Count:10
Flexural Modulus 1.10 - 2.00 GPa
160 - 290 ksi
Average value: 1.48 GPa Grade Count:10
Izod Impact, Notched 0.374 - 0.801 J/cm
0.700 - 1.50 ft-lb/in
Average value: 0.618 J/cm Grade Count:8
Izod Impact, Unnotched 8.01 - 5340 J/cm
15.0 - 10000 ft-lb/in
Average value: 11.3 J/cm Grade Count:6
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 49.0 - 77.8 °C
120 - 172 °F
Average value: 60.6 °C Grade Count:7
Flammability, UL94 HB
HB
Grade Count:4
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+11 - 1.00e+13 ohm-cm
1.00e+11 - 1.00e+13 ohm-cm
Average value: 3.70e+12 ohm-cm Grade Count:3
Processing Properties Metric English Comments
Processing Temperature 216 - 266 °C
420 - 510 °F
Average value: 244 °C Grade Count:5
Melt Temperature 221 - 274 °C
430 - 525 °F
Average value: 249 °C Grade Count:5
Mold Temperature 65.6 - 110 °C
150 - 230 °F
Average value: 86.3 °C Grade Count:8
Drying Temperature 75.0 - 105 °C
167 - 221 °F
Average value: 85.5 °C Grade Count:5
Moisture Content 0.100 %
0.100 %
Average value: 0.100 % Grade Count:3
Dew Point -40.0 °C
-40.0 °F
Average value: -40.0 °C Grade Count:3
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Average value: 86.2 MPa Grade Count:6