Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 225 °C | 437 °F | mass temp |
Lehmann & Voss LUVOCOM® TPU-7682 Thermoplastic polyurethane, with carbon fiber Applications: Electrically conductive, suitable for continuous discharging of statically generated electricity.Improved wear behaviour, low warpage.Bearings, sleeves, sliding elements, chair rollers.. |
|||
Processing Temperature | 225 °C | 437 °F | mass temp |
Lehmann & Voss LUVOCOM® 100-7126 VP Thermoplastic polyurethane, with PTFE Applications: Improved friction and wear behaviour. Emergency running property.dynamic stressBearings, sleeves, sliding elements, chair rollers, handles.Information provided by Lehmann & Voss & Co.K.. |
|||
Processing Temperature | 225 - 260 °C | 437 - 500 °F | |
Zhejiang Juner 301-G30 30% Glass Fibre Reinforced and Flammable Resistant Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Processing Temperature | 225 - 260 °C | 437 - 500 °F | |
Zhejiang Juner PA-A4 Flame-Retardant & Mineral Reinforced PA6 Applications: Top Grad CBInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Processing Temperature | 225 - 270 °C | 437 - 518 °F | |
Zhejiang Juner PC Alloy Applications: Shell of Small Household Electric ApplianceInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Processing Temperature | 225 °C | 437 °F | Film extrusion temperature |
Dow ATTANE™ 4301 Ultra Low Density Polyethylene, Blown Film Grade ATTANE® 4301 copolymer is an ultra low density polyethylene having high impact resistance and tear strength in blown films, designed for use in food packaging applications. It has low levels of sli.. |
|||
Processing Temperature | 225 °C | 437 °F | Film extrusion temperature |
Dow ATTANE™ 4501 Ultra Low Density Polyethylene, Blown Film Grade ATTANE® 4501 copolymer is an ultra low density polyethylene having high tear strength and impact resistance, designed for use in industrial/ consumer film applications, either as a high performance.. |
|||
Processing Temperature | 225 °C | 437 °F | Film extrusion temperature |
Dow ATTANE™ 4601 Ultra Low Density Polyethylene, Medical Packaging Grade ATTANE® 4601 copolymer is an ultra low density polyethylene blown film extrusion grade having high impact resistance and tear strength combined with improved softness, designed for use in medical p.. |
|||
Processing Temperature | 225 °C | 437 °F | Film extrusion temperature |
Dow ATTANE™ 4701 Ultra Low Density Polyethylene, Medical Packaging Grade ATTANE® 4701 copolymer is an ultra low density polyethylene having high pinhole and puncture resistance, tear strength and high impact resistance combined with improved softness. It has low levels .. |
|||
Processing Temperature | 225 °C | 437 °F | Recommended Extrusion Temperature |
Arkema Group Pebax® 6333 SA 01 MED Polyether Block Amide (PEBA) Polyether block amide PEBAX® 6333 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t.. |
|||
Processing Temperature | 225 °C | 437 °F | Recommended Extrusion Temperature |
Arkema Group Pebax® 6333 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 6333 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema .. |
|||
Processing Temperature | 225 °C | 437 °F | Recommended Extrusion Temperature |
Arkema Group Pebax® 6333 SP 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 6333 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide.. |
|||
Processing Temperature | 225 °C | 437 °F | Recommended Extrusion Temperature |
Arkema Group Pebax® 7233 SA 01 MED Polyether Block Amide (PEBA) Polyether block amide PEBAX® 7233 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t.. |
|||
Processing Temperature | 225 °C | 437 °F | Recommended Extrusion Temperature |
Arkema Group Pebax® Rnew 63R53 SP 01 Polyether Block Amide (PEBA) Polyether block amide Pebax® 63R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV.. |
|||
Processing Temperature | 225 - 245 °C | 437 - 473 °F | |
BASF Elastollan R 2001 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Processing Temperature | 225 - 245 °C | 437 - 473 °F | |
BASF Elastollan R 2002 25% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Processing Temperature | 225 - 245 °C | 437 - 473 °F | |
BASF Elastollan R 2005/1 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Processing Temperature | 225 - 245 °C | 437 - 473 °F | |
BASF Elastollan R 2006 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Processing Temperature | 225 - 245 °C | 437 - 473 °F | |
BASF Elastollan R 3000 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Processing Temperature | 225 - 245 °C | 437 - 473 °F | |
BASF Elastollan R 3001 15% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Processing Temperature | 225 °C | 437 °F | Approximate middle barrel temperature. |
A. Schulman ComAlloy Comtuf® 106 Polypropylene, Glass/Mineral Reinforced, Chemically Coupled, Impact Modified, UL Data provided by the manufacturer, ComAlloy International Company.30% Glass/Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has .. |
|||
Processing Temperature | 225 °C | 437 °F | Approximate middle barrel temperature. |
A. Schulman ComAlloy Hiloy® 119 Polypropylene, Glass/Mineral Reinforced, Chemically Coupled Data provided by the manufacturer, ComAlloy International Company.30% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Processing Temperature | 225 °C | 437 °F | Approximate middle barrel temperature. |
A. Schulman ComAlloy Hiloy® 131 Polypropylene, Glass/Mineral Reinforced, Chemically Coupled Data provided by the manufacturer, ComAlloy International Company.50% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Processing Temperature | 225 - 245 °C | 437 - 473 °F | |
BASF Elastollan R 1001 10% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Processing Temperature | 225 - 245 °C | 437 - 473 °F | |
BASF Elastollan R 2000 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Processing Temperature | 225 °C | 437 °F | Approximate middle barrel temperature. |
A. Schulman ComAlloy Hiloy® 132 Polypropylene, Glass/Mineral Reinforced, Chemically Coupled Data provided by the manufacturer, ComAlloy International Company.45% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Processing Temperature | 225 - 270 °C | 437 - 518 °F | |
Zhejiang Juner PC-3-1 Alloy Applications: Shell of Small Household Electric ApplianceInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Processing Temperature | 225 - 250 °C | 437 - 482 °F | |
Zhejiang Juner PA-A6-6H High CTI Value Halogen-Free Environmental Protection Flame-Resistant and Reinforced Polyamide Applications: Circuit Breaker, BaseInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Processing Temperature | 225 - 270 °C | 437 - 518 °F | |
Zhejiang Juner PC/ABSz-4 Alloy Applications: Shell of Small Household Electric ApplianceInformation provided by Zhejiang Juner New Materials Co, Ltd. |