Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lehmann & Voss LUVOCOM® 100-7846 Thermoplastic polyurethane, with aramid reinforcement

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 100-7846 Thermoplastic polyurethane, with aramid reinforcement.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Improved friction and wear behaviour. Emergency running property.dynamic stressBearings, sleeves, sliding elements, chair rollers, handles.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ISO 1183
Water Absorption <= 0.30 %
<= 0.30 %
23°C/24h
Linear Mold Shrinkage 0.015 - 0.020 cm/cm
0.015 - 0.020 in/in
Mechanical Properties Metric English Comments
Tensile Stress 25.0 MPa
3630 psi
Elongation at Yield 650 %
650 %
Modulus of Elasticity 0.0500 GPa
7.25 ksi
Charpy Impact, Notched 2.30 J/cm²
10.9 ft-lb/in²
ISO 179 1eA
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 90.0 °C
194 °F
110 °C
230 °F
short term
Electrical Properties Metric English Comments
Surface Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
Insulation Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
Processing Properties Metric English Comments
Processing Temperature 225 °C
437 °F
mass temp
Nozzle Temperature 210 - 230 °C
410 - 446 °F
Zone 1 210 - 230 °C
410 - 446 °F
Zone 2 210 - 230 °C
410 - 446 °F
Zone 3 210 - 230 °C
410 - 446 °F
Mold Temperature 25.0 - 60.0 °C
77.0 - 140 °F
Drying Temperature 60.0 - 90.0 °C

@Time 7200 - 10800 sec
140 - 194 °F

@Time 2.00 - 3.00 hour
Dehumidifying dryer
100 - 110 °C

@Time 7200 - 10800 sec
212 - 230 °F

@Time 2.00 - 3.00 hour
Air-Circulation Dryer
Descriptive Properties Value Comments
Color natural color (yellow)