Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 40.0 - 50.0 MPa | 5800 - 7250 psi | Average value: 45.0 MPa Grade Count:5 |
Overview of materials for Nylon 12, Extrusion/Tubing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Extrusion/Tubing Grade". Each property range of values reported is minimum and maximum values .. |
|||
Injection Pressure | 40.0 - 50.0 MPa | 5800 - 7250 psi | Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.) |
UBE UBESTA® 3014U Rigid Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Injection Pressure | 40.0 - 50.0 MPa | 5800 - 7250 psi | Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.) |
UBE UBESTA® 3020IX1 Rigid Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: conductive, impact modifiedInformation provided by UBE. |
|||
Injection Pressure | 40.0 - 50.0 MPa | 5800 - 7250 psi | Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.) |
UBE UBESTA® 3020X15 Nylon 12 Thermister Description: UBESTA Nylon 12 ThermisterInformation provided by UBE. |
|||
Injection Pressure | 40.0 - 50.0 MPa | 5800 - 7250 psi | Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.) |
UBE UBESTA® 3020X8 Nylon 12 Thermister Description: UBESTA Nylon 12 ThermisterInformation provided by UBE. |
|||
Injection Pressure | 40.0 - 50.0 MPa | 5800 - 7250 psi | Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.) |
UBE UBESTA® 3024LU Rigid Black Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Injection Pressure | 40.0 - 50.0 MPa | 5800 - 7250 psi | Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.) |
UBE UBESTA® 3024NUX Short Cycle Time Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Injection Pressure | 40.0 - 50.0 MPa | 5800 - 7250 psi | Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.) |
UBE UBESTA® 3024U Rigid Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Injection Pressure | 40.0 - 50.0 MPa | 5800 - 7250 psi | Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.) |
UBE UBESTA® 3030JI44 Plasticized Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: ultra flexible, low migrationInformation provided by UBE. |
|||
Injection Pressure | 40.0 - 50.0 MPa | 5800 - 7250 psi | Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.) |
UBE UBESTA® 3030JI5L 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, impact modified and stabilized against weatherability (DIN 73378 Nomenclature = PA12 HIPHL)Information provided by U.. |
|||
Injection Pressure | 40.0 - 50.0 MPa | 5800 - 7250 psi | Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.) |
UBE UBESTA® 3030JI5L Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: meet SAE J844, DIN73378 HIPHLInformation provided by UBE. |
|||
Injection Pressure | 40.0 - 50.0 MPa | 5800 - 7250 psi | Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.) |
UBE UBESTA® 3030JI7 Plasticized Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: low migrationInformation provided by UBE. |
|||
Injection Pressure | 40.0 - 50.0 MPa | 5800 - 7250 psi | Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.) |
UBE UBESTA® 3030JLX1 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, stabilized against weatherability (DIN 73378 Nomenclature = PA12 PHL)Information provided by UBE. |
|||
Injection Pressure | 40.0 - 50.0 MPa | 5800 - 7250 psi | Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.) |
UBE UBESTA® 3030JLX1 Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE. |
|||
Injection Pressure | 40.0 - 50.0 MPa | 5800 - 7250 psi | Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.) |
UBE UBESTA® 3030JLX2 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, stabilized against weatherability Information provided by UBE. |
|||
Injection Pressure | 40.0 - 50.0 MPa | 5800 - 7250 psi | Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.) |
UBE UBESTA® P3014UMX Powder Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Injection Pressure | 2.00 - 50.0 MPa | 290 - 7250 psi | Melt Pressure |
Wacker Silicones Geniomer® 140 Silicone TPE SLM TPSE 140 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phas.. |
|||
Injection Pressure | 40.0 - 50.0 MPa | 5800 - 7250 psi | |
Toyobo GLAMIDE® T-714E Transparent Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Injection Pressure | 40.0 - 50.0 MPa | 5800 - 7250 psi | |
Toyobo GLAMIDE® T-777-02 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Injection Pressure | 40.0 - 50.0 MPa | 5800 - 7250 psi | Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.) |
UBE UBESTA® 3030JI6L Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: for multilayer tubeInformation provided by UBE. |
|||
Injection Pressure | 40.0 - 50.0 MPa | 5800 - 7250 psi | Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.) |
UBE UBESTA® 3030JLX2 Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: semi-plasticized, UV resistance, heat resistanceInformation provided by UBE. |
|||
Injection Pressure | 40.0 - 50.0 MPa | 5800 - 7250 psi | Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.) |
UBE UBESTA® 3030UFX1 Rigid Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE. |
|||
Injection Pressure | 40.0 - 50.0 MPa | 5800 - 7250 psi | Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.) |
UBE UBESTA® 3030XA Nylon 12 Film Description: UBESTA Nylon 12 FilmInformation provided by UBE. |
|||
Injection Pressure | 40.0 - 50.0 MPa | 5800 - 7250 psi | Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.) |
UBE UBESTA® 3035JU5 Plasticized Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: ultra flexible, heat resistanceInformation provided by UBE. |
|||
Injection Pressure | 40.0 - 50.0 MPa | 5800 - 7250 psi | Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.) |
UBE UBESTA® 3035LU1 Rigid Piping Grade Nylon 12 Description: UBESTA contributes to the field of Utilities such as plastic pipe system evolutionary developed for gas industry. It is used for both burial and for rehabilitation of existing cast iron.. |
|||
Injection Pressure | 40.0 - 50.0 MPa | 5800 - 7250 psi | Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.) |
UBE UBESTA® 3035UF Rigid Piping Grade Nylon 12 Description: UBESTA contributes to the field of Utilities such as plastic pipe system evolutionary developed for gas industry. It is used for both burial and for rehabilitation of existing cast iron.. |
|||
Injection Pressure | 40.0 - 50.0 MPa | 5800 - 7250 psi | Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.) |
UBE UBESTA® 3030LUX 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: rigid, stabilized against weatherability (DIN 73378 Nomenclature = PA12 HL)Information provided by UBE. |
|||
Injection Pressure | 40.0 - 50.0 MPa | 5800 - 7250 psi | Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.) |
UBE UBESTA® 3035JX47 Plasticized Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: conductiveInformation provided by UBE. |
|||
Injection Pressure | 2.00 - 50.0 MPa | 290 - 7250 psi | Melt Pressure |
Wacker Silicones Geniomer® 80 Silicone TPE SLM TPSE 80 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phase.. |
|||
Injection Pressure | 2.00 - 50.0 MPa | 290 - 7250 psi | Melt Pressure |
Wacker Silicones Geniomer® 60 Silicone TPE SLM TPSE 60 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phase.. |