Processing Properties Metric English Comments
Pot Life 10 - 15 min
10 - 15 min
Mass: 50g
Resinlab® EP1112 Clear Electronic Grade Epoxy Encapsulant
Resinlab™ EP 1112 Clear is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexib..
Pot Life 8.0 - 15 min
8.0 - 15 min
Time before parts must be mated
Lord Adhesives 7542C Two-Component Urethane Adhesive
Lord Urethane AdhesivesLord® one- and two-part urethane adhesives provide superior bonds with minimal surface preparation for today's high performance thermosets and thermoplastics. They offe..
Pot Life 12 - 15 min
12 - 15 min
ITW Plexus Plexusâ„¢ MA3940 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Use with craze sensitive plastics.Information provided by Illinois Tool Works.
Pot Life 10 - 15 min
10 - 15 min
100 gram batch
Master Bond EP41S Fast Curing Epoxy Features Chemical Resistance
Description: Master Bond EP41S is a two component epoxy resin compound for durable, high performance, tough, high strength coatings, liners and sealants with outstanding resistance to organic solven..
Pot Life 10 - 15 min
10 - 15 min
100 gram mass
Master Bond EP41SMed Two Component, Low Viscosity, USP Class VI Epoxy System
Master Bond Polymer Adhesive EP41S Medical is a two component low viscosity epoxy resin system for high performance bonding, sealing, coating, as well as small encapsulations, pottings and castings...
Pot Life 14 - 15 min

@Temperature 24.0 °C
14 - 15 min

@Temperature 75.2 °F
1/2 lb mass
BCC Products BC 5003 Epoxy Laminating System
BC 5003 is a medium viscosity, unfilled laminating system. It is a room temperature curing resin with a relatively short pot life. BC 5003 is also considered an excellent general purpose adhesive fo..
Pot Life 12 - 15 min

@Temperature 24.0 °C
12 - 15 min

@Temperature 75.2 °F
BCC Products BC 8880 Polyurethane Elastomer Surface Coat
BC8880 is a two-part urethane gel coat which exhibits excellent handling characteristics and very low moisture sensitivity. Its characteristics include a high modulus and a high hardness. It is a br..
Pot Life 10 - 15 min
10 - 15 min
Mass: 50g
Resinlab® EP1112 Black Electronic Grade Epoxy Encapsulant
Resinlab™ EP 1112 Black is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexib..
Pot Life 10 - 15 min
10 - 15 min
Mass: 50g; TM R050-19
Resinlab® EP1305 Black Highly Toughened Urethane Modified Epoxy
Resinlab™ EP1305 Black is a highly toughened urethane modified epoxy designed for bonding PVC, metals, ceramics and other difficult to bond substrates. The system has a thixotropic non-sag viscosi..