Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Feed Temperature = 205 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Feed Temperature 190 - 205 °C
374 - 401 °F
Lubrizol Estane® S198A Thermoplastic Polyurethane
Type: Estane® S198A is a Shore 98A, polyester grade thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Americas, Europe, Middle East, ..
Copyright © lookpolymers.com All Rights Reserved