Processing Properties | Metric | English | Comments |
---|---|---|---|
Feed Temperature | 190 - 205 °C | 374 - 401 °F | |
Lubrizol Estane® S198A Thermoplastic Polyurethane Type: Estane® S198A is a Shore 98A, polyester grade thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Americas, Europe, Middle East, .. |