Polymer Property : Feed Temperature = 284 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Feed Temperature 140 - 150 °C
284 - 302 °F
Petroquimica Triunfo Trithene® TS 7028 LDPE - Automatic Packaging
The Trithene TS 7028 resin is a low-density polyethylene (LDPE) with excellent optical and processability properties that allows for the production of films combining appearance, mechanical strength..
Feed Temperature 140 - 150 °C
284 - 302 °F
Petroquimica Triunfo Tritheva® TN 2007 EVA Copolymer
The Tritheva TN 2007 resin is an Ethylene-Vinyl Acetate copolymer (EVA), developed to meet the multi-layer packaging needs where are required high strength, with high toughness, and excellent optica..
Feed Temperature 140 - 150 °C
284 - 302 °F
Petroquimica Triunfo Tritheva® TN 8093 EVA Copolymer
The Tritheva TN 8093 resin is a fractional MI copolymer of Ethylene-Vinyl Acetate (EVA), developed to meet the multi-layer and blending film applications where are required high strength, with high ..
Feed Temperature 140 °C
284 °F
Extrusion
Huntsman IROGRAN® PS455-200 TPU-Polyester
Introduction: IROGRAN PS455-200 is a polyester based thermoplastic polyurethane intended for extrusion applications. IROGRAN PS455-200 is part of the HUNTSMAN film and sheet product range and offers..
Feed Temperature 140 °C
284 °F
Extrusion Coating
DuPont™ Appeel® 11D888 Ethylene Vinyl Acetate
Appeel®11D888 is a developmental modified ethylene vinyl acetate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a ..
Feed Temperature 140 °C
284 °F
Blown Film Coextrusion
DuPont™ Appeel® 20D828 Ethylene Acrylate
Appeel® 20D828 is an modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide strong peelable seals over a broad temp..
Feed Temperature 140 °C
284 °F
Blown Film Coextrusion
DuPont™ Appeel® 20D855 Ethylene Acrylate
DuPont™ Appeel 20D855 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad tempe..
Feed Temperature 140 °C
284 °F
Blown Film Coextrusion
DuPont™ Appeel® 20D867 Ethylene Acrylate
DuPont™ Appeel 20D867 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad tempe..
Feed Temperature 140 °C
284 °F
Blown Film Coextrusion
DuPont™ Appeel® 20D875 Ethylene Acrylate
Appeel® 20D875 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide strong peelable seals over a broad tempe..
Feed Temperature 140 °C
284 °F
Blown Film Coextrusion
DuPont™ Appeel® 22D843 Ethylene Acrylate
DuPont™ Appeel® 22D843 is a polypropylene modified ethylene acrylate resin designed to function as a masterbatch to achieve peelability in polypropylene based sealant layers. It provides peelable ..
Feed Temperature 140 °C
284 °F
Blown Film Coextrusion
DuPont™ Appeel® 45D747 Polyolefin
Appeel® 45D747 is a modified polyolefin resin designed to provide easy peel functionality from polyethylene copolymers. Appeel® 45D747 is available in pellet form for use in conventional extrusion..
Feed Temperature 140 °C
284 °F
Blown Film Coextrusion
DuPont™ Appeel® 72D727 Sealing Resin
DuPont™ Appeel® 72D727 is a blown or cast film resin designed to be a sealing layer to film or sheet lidding applications. It provides a peelable seal to a number of materials including HDPE, LLDP..
Feed Temperature 140 °C
284 °F
Blown Film Coextrusion
DuPont™ Appeel® 20D784 Ethylene Acrylate
Appeel® 20D784 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad temperature ..