Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 160 - 175 °C | 320 - 347 °F | Extrusion Molding |
Kolon ELLAS K-260D Thermoplastic Polyurethane ApplicationsExtrusion: Antenna, Heel TipInjection: Hose, Tube, SheetIndustry Parts Information provided by API-Kolon. |
|||
Zone 1 | 160 - 175 °C | 320 - 347 °F | Injection Molding |
Kolon ELLAS K-296AB Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjection: Pneumatic tube, film/sheet, cableTransparent HoseIndustry Parts Information provided by API-Kolon. |
|||
Zone 1 | 155 - 175 °C | 311 - 347 °F | Extrusion Molding |
Kolon ELLAS K-385A Ether Based Thermoplastic Polyurethane ApplicationsExtrusionInjection: Cable Sheathing, High pressure tubeWheelCaster Information provided by API-Kolon. |
|||
Zone 1 | 160 - 175 °C | 320 - 347 °F | Injection Molding |
Kolon ELLAS K-385A Ether Based Thermoplastic Polyurethane ApplicationsExtrusionInjection: Cable Sheathing, High pressure tubeWheelCaster Information provided by API-Kolon. |
|||
Zone 1 | 155 - 175 °C | 311 - 347 °F | Extrusion Molding |
Kolon ELLAS K-390A Ether Based Thermoplastic Polyurethane ApplicationsExtrusion: Cable Sheathing, high pressure tubeInjectionElectric WireIndustry Parts Information provided by API-Kolon. |
|||
Zone 1 | 160 - 175 °C | 320 - 347 °F | Injection Molding |
Kolon ELLAS K-395A Ether Based Thermoplastic Polyurethane ApplicationsExtrusionInjection: Cable sheathing, Highly Pressurized HoseIndustry Parts Information provided by API-Kolon. |
|||
Zone 1 | 155 - 175 °C | 311 - 347 °F | Extrusion Molding |
Kolon ELLAS K-395F Ether Based Thermoplastic Polyurethane ApplicationsExtrusionHighly Pressurized Hose Information provided by API-Kolon. |
|||
Zone 1 | 155 - 175 °C | 311 - 347 °F | Injection Molding |
Kolon ELLAS K-429A Ester Based Thermoplastic Polyurethane ApplicationsIndustry PartsOutsole of Soccer ShoeHighly Pressurized Hose Information provided by API-Kolon. |
|||
Zone 1 | 155 - 175 °C | 311 - 347 °F | Injection Molding |
Kolon ELLAS K-475A Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionIndustry PartsParts for Automobile/Mobile phoneInformation provided by API-Kolon. |
|||
Zone 1 | 160 - 175 °C | 320 - 347 °F | Injection Molding |
Kolon ELLAS K-585A Caprolactone Based Thermoplastic Polyurethane ApplicationsInjectionIndustry Parts Information provided by API-Kolon. |
|||
Zone 1 | 155 - 175 °C | 311 - 347 °F | Extrusion Molding |
Kolon ELLAS K-596A Caprolactone Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionDust SealOil Seal Information provided by API-Kolon. |
|||
Zone 1 | 155 - 175 °C | 311 - 347 °F | Extrusion Molding |
Kolon ELLAS K-787A Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionFlexible HoseIndustry Parts Information provided by API-Kolon. |
|||
Zone 1 | 160 - 175 °C | 320 - 347 °F | Extrusion Molding |
Kolon ELLAS K-792A Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionFlexible HoseIndustry Parts Information provided by API-Kolon. |
|||
Zone 1 | 160 - 175 °C | 320 - 347 °F | Injection Molding |
Kolon ELLAS K-796A Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionPneumatic HoseTransparent HoseIndustry Parts Information provided by API-Kolon. |