Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 195 °C | 383 °F | |
Lubrizol Advanced Materials Pearlthane® 11T85 Polycaprolactone Copolyester based TPU Type : Pearlthane® 11T85 is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Adequate hardness, excellent mechanical propert.. |
|||
Zone 1 | 195 °C | 383 °F | |
Lubrizol Advanced Materials PEARLTHANE® 11T95P Thermoplastic Polyurethane Elastomer Type : Pearlthane® 11T95P is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining hardness with excellent mechanical p.. |
|||
Zone 1 | 195 °C | 383 °F | Compression Zone |
Lubrizol Advanced Materials PEARLTHANE® D11H92S Thermoplastic Polyurethane Elastomer PEARLTHANE® D11H92S is a high performance polycaprolactone copolyester based TPU, supplied in form of translucent, colorless pellets, featuring excellent flow and mechanical properties and an out.. |
|||
Zone 1 | 195 °C | 383 °F | Extrusion Blow Molding |
SK Chemicals SKYGREEN® PETG 2008 Specially Formulated PET Copolymer Resin SKYGREEN PETG is an amorphous copolyester in which a certain amount of ethylene glycol is replaced with 1,4-cyclohexane dimethanol (CHDM), which prevent crystallization, leading to improved processa.. |
|||
Zone 1 | 195 - 205 °C | 383 - 401 °F | Injection |
Lubrizol Estane® GP 55 DB Thermoplastic Polyurethane Type: Estane® GP 55DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Features: Translucent spherical pellets.Uses: Injection molding partsAvailable in EuropeInformation Provided by.. |
|||
Zone 1 | 195 - 205 °C | 383 - 401 °F | Injection |
Lubrizol ESTANE® GP52DB Ester Based Thermoplastic Polyurethane Type: Estane® GP 52DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Zone 1 | 195 - 205 °C | 383 - 401 °F | Injection |
Lubrizol ESTANE® GP95AB Ester Based Thermoplastic Polyurethane Type: Estane® GP 95AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tagsAvailable in .. |
|||
Zone 1 | 195 - 205 °C | 383 - 401 °F | |
Eurostar Starglas FF001 HDPE, Glass Fiber Filled Starglas FF001 is a Glass Fiber Reinforced High Density Polyethylene ResinInformation provided by Eurostar. |
|||
Zone 1 | 195 - 205 °C | 383 - 401 °F | |
Eurostar Starpylen HU 70E3 HDPE, Injection Molding Starpylen HU 70E3 is a High Density Polypropylene Injection Molding Resin (also known as HU70E3)Information provided by Eurostar. |
|||
Zone 1 | 195 - 205 °C | 383 - 401 °F | |
Eurostar Starpylen HW 30K ECR-BK PP, Injection Molded Starpylen HW 30K ECR-BK is a reinforced Polypropylene with a low carbon footprint spherical filler, Injection Molding Resin (also known as HW30KECR)Information provided by Eurostar. |
|||
Zone 1 | 195 - 205 °C | 383 - 401 °F | |
Eurostar Starpylen HZ 50E3 PP, Injection Molded PRELIMINARY-Starpylen HZ 50E3 is a High Specific Gravity Polypropylene (density 1.5), Injection Molding Resin (also known as HZ50E3)Information provided by Eurostar. |
|||
Zone 1 | 195 - 205 °C | 383 - 401 °F | |
Eurostar Starpylen HZ 80E7 HDPE, Injection Molding Starpylen HZ 80E7 is a High Specific Gravity Polypropylene, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 195 - 205 °C | 383 - 401 °F | |
Eurostar Starpylen MB006SU PP, Glass Bead Filled, Injection Molding Resin Starpylen MB006SU is a Glass Bead Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 195 - 205 °C | 383 - 401 °F | |
Eurostar Starpylen MCR13S PP, 15% Carbon Fiber Filled, Injection Molded Starpylen MCR13S is a 15% Carbon Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 195 - 205 °C | 383 - 401 °F | |
Eurostar Starpylen MF003SU PP, 15% Glass Fiber Filled, Injection Molded Starpylen MF003SU is a 15% Glass Fiber Reinforced Polypropylene Injection Molding Resin (also known as Starpylen WX 15V S34/040)Information provided by Eurostar. |
|||
Zone 1 | 195 - 205 °C | 383 - 401 °F | |
Eurostar Starpylen MF004S PP, 20% Glass Fiber Filled, Injection Molded Starpylen MF004S is a 20% Glass Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 195 - 205 °C | 383 - 401 °F | |
Eurostar Starpylen MFB44S PP, Glass Bead/Glass Fiber Filled Starpylen MFB44S is a Glass Beads, Glass Fiber Reinforced, Polypropylene Injection Molding Resin heat stabilized (also known as Starpylen WS 2020VK S37.7)Information provided by Eurostar. |
|||
Zone 1 | 195 - 205 °C | 383 - 401 °F | |
Eurostar Starpylen MFK42AS PP, Glass/Mineral Filled, Injection Molded Starpylen MFK42AS is a Mineral Filled, Glass Fiber Reinforced, Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 195 - 205 °C | 383 - 401 °F | |
Eurostar Starpylen MFM43S PP, Glass/Mineral Filled, Injection Molded Starpylen MFM43S is a Mineral Filled, Glass Fiber Reinforced, Polypropylene Injection Molding Resin, also recognized as Starpylen WV 30VMC S37/7 Black 301Information provided by Eurostar. |
|||
Zone 1 | 195 - 205 °C | 383 - 401 °F | |
Eurostar Starpylen MH0200A HDPE, Injection Molding Starpylen MH0200A is a High Density Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 195 - 205 °C | 383 - 401 °F | |
Eurostar Starpylen MK001AS PP, Mineral Filled, Injection Molding Starpylen MK001AS is a Mineral Filled Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 195 - 205 °C | 383 - 401 °F | |
Eurostar Starpylen MX05038 TPEX, Injection Molded Starpylen MX05038 is a TPEX Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 195 - 205 °C | 383 - 401 °F | |
Eurostar Starpylen MX06023 PP, 20% Milled Glass Fiber Filled, Injection Molded Starpylen MX06023 is a 20% Milled Glass Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 195 - 205 °C | 383 - 401 °F | |
Eurostar Starpylen MX06050 PP, 30% Glass Filled, Injection Molded Starpylen MX06050 is a 30% Glass Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 195 - 205 °C | 383 - 401 °F | |
Eurostar Starglas FX05032 PE Starglas FX05032 is Polyethylene Resin with a Proprietary Additive (foaming agent for polyolefins)Information provided by Eurostar. |
|||
Zone 1 | 195 °C | 383 °F | Extrusion |
Alliance Polymers Zythane™ 5050D Thermoplastic Polyurethane Elastomer Zythane™ 5050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Zone 1 | 195 °C | 383 °F | Extrusion |
Alliance Polymers Zythane™ 7050D Thermoplastic Polyurethane Elastomer Zythane™ 7050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Zone 1 | 195 °C | 383 °F | Extrusion |
Alliance Polymers Viprene™ G50D-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G50D-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Zone 1 | 195 °C | 383 °F | |
Lubrizol Advanced Materials PEARLTHANE® 11T93 Thermoplastic Polyurethane Elastomer Type : Pearlthane® 11T93 is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining hardness with excellent mechanical prop.. |
|||
Zone 1 | 195 - 205 °C | 383 - 401 °F | Injection |
Lubrizol Estane® GP 52 DT Thermoplastic Polyurethane Type: Estane® GP 52DT is an aromatic polyester-based thermoplastic polyurethane (TPU).Features: Translucent spherical pellets.Uses: Injection molding parts, animal identification tagsAvailable in E.. |