Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eurostar Starpylen HZ 50E3 PP, Injection Molded

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Eurostar Engineering Plastics
Trade Name Starpylen
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurostar Starpylen HZ 50E3 PP, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PRELIMINARY-Starpylen HZ 50E3 is a High Specific Gravity Polypropylene (density 1.5), Injection Molding Resin (also known as HZ50E3)Information provided by Eurostar.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183
Melt Flow 24 g/10 min

@Load 2.16 kg,
Temperature 230 °C
24 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.0 MPa
3190 psi
ISO 527
Elongation at Break 27 %
27 %
ISO 527
Flexural Strength 36.0 MPa
5220 psi
ISO 178
Flexural Modulus 2.30 GPa
334 ksi
ISO 178
Izod Impact, Notched (ISO) 2.90 kJ/m²
1.38 ft-lb/in²
80x10x4; ISO 180/1A
Izod Impact, Unnotched (ISO) 28.0 kJ/m²
13.3 ft-lb/in²
80x10x4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 61.0 °C
142 °F
Flatw 80x10x4, sp=64 mm; ISO 75/Af
Processing Properties Metric English Comments
Zone 1 195 - 205 °C
383 - 401 °F
Zone 2 215 - 225 °C
419 - 437 °F
Zone 3 225 - 250 °C
437 - 482 °F
Melt Temperature 225 - 250 °C
437 - 482 °F
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Drying Temperature 70.0 °C

@Time 10800 sec
158 °F

@Time 3.00 hour