Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 185 - 200 °C | 365 - 392 °F | |
Lubrizol Advanced Materials PEARLTHANE® 16N85UV Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 16N85UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of translucent, colorless, combining hardness with excellent mechanical properties and excellent hydro.. |
|||
Zone 1 | 180 - 200 °C | 356 - 392 °F | Blow Molding |
LG Chemical BM662 ABS, Heat Resistance Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical.. |
|||
Zone 1 | 180 - 200 °C | 356 - 392 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 1040D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Zone 1 | 190 - 200 °C | 374 - 392 °F | Extrusion Molding |
LG Chemical LI968W Co-Extrusion ASA Description: Good WeatherabilityApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Zone 1 | 190 - 200 °C | 374 - 392 °F | Extrusion Molding |
LG Chemical LI970 Co-Extrusion ASA Description: Good Weatherability, Scratch ResistanceApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Zone 1 | 190 - 200 °C | 374 - 392 °F | Extrusion Molding |
LG Chemical LI970HF Co-Extrusion ASA Description: Good Weatherability, Scratch Resistance, High FlowApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Zone 1 | 190 - 200 °C | 374 - 392 °F | |
Lubrizol Advanced Materials PEARLTHANE® 11T92E Thermoplastic Polyurethane Elastomer Type: Pearlthane® 11T92E is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Extrusion/MouldingSpecial Features : Combining hardness with excellent mechanical pr.. |
|||
Zone 1 | 170 - 200 °C | 338 - 392 °F | |
Lubrizol Advanced Materials PEARLTHANE® 11T98 Thermoplastic Polyurethane Elastomer PEARLTHANE® 11T98 is a polycaprolactone copolyester based TPU, supplied in form of translucent, colorless pellets, combining high hardness with excellent mechanical properties. It can be extruded.. |
|||
Zone 1 | 185 - 200 °C | 365 - 392 °F | |
Lubrizol Advanced Materials PEARLTHANE® Clear 15N85 Thermoplastic Polyurethane Elastomer Type : Pearlthane® CLEAR 15N85 is a polyether copolymer-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Outstanding colour, a very low yellowness index as.. |
|||
Zone 1 | 180 - 200 °C | 356 - 392 °F | Extrusion Molding |
LG Chemical MA221 ABS, High Impact, Low Gloss Feature: Injection Molding, Extrusion Molding, High Impact, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |
|||
Zone 1 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Catalyst CAT 10 Polyolefin Catalyst CAT 10 is a high density based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to.. |
|||
Zone 1 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Catalyst CT 0552/09 Polyolefin Catalyst CT 0552/09 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water.. |
|||
Zone 1 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Catalyst LV/1LR Polyolefin Catalyst LV/1LR is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or .. |
|||
Zone 1 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Catalyst PS/2 Polyolefin Catalyst PS/2 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that take place by exposure of the pipe to water or steam .. |
|||
Zone 1 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Catalyst PS/2 UV Polyolefin Catalyst PS/2 UV is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or.. |
|||
Zone 1 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Catalyst PS/2LRO Polyolefin Catalyst PS/2LR0 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or.. |
|||
Zone 1 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Catalyst PS/4 Polyolefin Catalyst PS/4 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or st.. |
|||
Zone 1 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Polidan® PNT 0553/23 Polyethylene, Crosslinked (XLPE) POLIDAN® PNT 0553/23 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction.Features: Crosslinkable; Good Flexibility; Lo.. |
|||
Zone 1 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Polidan® PNT 0555/06 Polyethylene, Crosslinked (XLPE) POLIDAN® PNT 0555/06 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes... |
|||
Zone 1 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Polidan® T/A Polyethylene, Crosslinked (XLPE) POLIDAN® T/A is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Features.. |
|||
Zone 1 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Polidan® T/A-HF Polyethylene, Crosslinked (XLPE) POLIDAN® T/A-HF is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu.. |
|||
Zone 1 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Polidan® T/A-LV Polyethylene, Crosslinked (XLPE) POLIDAN® T/A-LV is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu.. |
|||
Zone 1 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Polidan® T/A-LX Polyethylene, Crosslinked (XLPE) POLIDAN® T/A-LX is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu.. |
|||
Zone 1 | 190 - 200 °C | 374 - 392 °F | |
Eurostar Starpylen HU 30E4 ECR PP, Mineral Filled, Injection Molding Starpylen HU 30E4 ECR is a reinforced Polypropylene with a low carbon footprint renewable mineral filler, Injection Molding Resin (also known as HUS30E4ECR)Information provided by Eurostar. |
|||
Zone 1 | 190 - 200 °C | 374 - 392 °F | |
Lubrizol Advanced Materials Pearlthane® ECO D20N88 Thermoplastic Polyurethane
(discontinued **) PEARLTHANE® ECO D20N88 is a 86 Shore A, High Performance natural TPU based on Renewable Sources with ca. 60% renewable content according to ASTM D6866 for Extrusion and Injection Molding applicatio.. |
|||
Zone 1 | 190 - 200 °C | 374 - 392 °F | Extrusion Molding |
LG Chemical LI923 Extrusion ASA Description: Good Weatherability, High RigidityApplication: Communication Instrument Cover, Cable Connecting Cover, Door PanelCAS: 26299-47-8Information provided by LG Chemical |