Processing Properties Metric English Comments
Zone 1 340 - 360 °C
644 - 680 °F
Lehmann & Voss LUVOCOM® 1500-0871 Polysulfone, with glass spheres
Applications: Isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precision parts, high continuous use temperature.Control disks, ca..
Zone 1 340 - 360 °C
644 - 680 °F
Lehmann & Voss LUVOCOM® 1500-8299 Polysulfone, with PTFE, lubricant modified
Applications: Isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precision parts, high continuous use temperature.Control disks, ca..
Zone 1 340 °C
644 °F
Feed zone
BASF Ultrason® E 2010 MR SW 10111 PESU
Description: Unreinforced, medium viscosity standard injection molding grade, demolding optimized. Abbreviated designation according to ISO 1043-1: PESU.Information provided by BASF
Zone 1 340 °C
644 °F
Feed zone
BASF Ultrason® E 2010 HC PESU
Information provided by BASF
Zone 1 340 °C
644 °F
Feed zone
BASF Ultrason® E 2010 MR HP PESU
Description: Unreinforced, medium viscosity standard injection molding grade for improved demolding behavior with Mold Release. PES-Blend with improved processibility. (High Productivity) Abbreviate..
Zone 1 340 °C
644 °F
Feed zone
BASF Ultrason® E 2010 SW Q31 10088 PESU
Information provided by BASF