Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® OBC 4665A Thermoplastic Elastomer Uses: Blow Molding Applications; General Purpose; Soft Touch Applications Forms: Pellets Processing Method: Blow Molding; Profile Extrusion; Sheet Extrusion; Thermoforming; Wire and Cable Extrusion;.. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL EF-6123 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL EF-6162 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1017A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1050-75 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1138 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1154A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1182A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1420C Thermoplastic Elastomer Uses: Consumer Applications; Flexible Grips; General Purpose; Grommets; Industrial Soft; Sporting Goods; Toys; Weatherstripping Forms: Pellets Processing Method: Extrusion; Injection Molding Injecti.. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1431F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1654B Thermoplastic Elastomer Notes: Non-halogenated Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstr.. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1654G Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1686D Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1934A BLK 111 Thermoplastic Elastomer Information Provided by Teknor Apex |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1934C Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-2363B Thermoplastic Elastomer Availability: North America Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weath.. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-2560A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-2563A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-2575A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-2588L Thermoplastic Elastomer Uses: Consumer Applications; Flexible Grips; General Purpose; Handles; Personal Care; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-F.. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-2717B Thermoplastic Elastomer Uses: Consumer Applications; Flexible Grips; General Purpose; Grommets; Industrial Soft; Sporting Goods; Toys; Weatherstripping Forms: Pellets Processing Method: Extrusion; Injection Molding Inject.. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-3954-80 Thermoplastic Elastomer Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire .. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-4001 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-87-L832-B Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-94-T1422A-100 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec.. |
|||
Zone 2 | 171 - 210 °C | 340 - 410 °F | |
Teknor Apex Uniprene® UN-1140A Thermoplastic Elastomer Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Zone 2 | 171 - 210 °C | 340 - 410 °F | |
Teknor Apex Uniprene® UN-2467A Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Zone 2 | 171 - 210 °C | 340 - 410 °F | |
Teknor Apex Uniprene® UN-7100-87 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Zone 2 | 171 °C | 340 °F | Extrusion |
Lubrizol ESTANE® 58300 Ether Based Thermoplastic Polyurethane Features: Good physical properties, hydrolysis resistance, low temperature performance and abrasion with a wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injectio.. |
|||
Zone 2 | 171 - 210 °C | 340 - 410 °F | |
Teknor Apex Uniprene® UN-7100-50D Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |