Material Notes:
Surlyn® 1706 is available for use in conventional blown, cast film, and sheet extrusion equipment. It is also used in coextrusion equipment designed to process polyethylene and ethylene copolymer type resins. SURLYN® 1706 complies with Food and Drug Administration Regulation 21 CFR 177.1330(a) - - Ionomeric resins, subject to the limitations and requirements therein. This Regulation describes polymers that may be used in contact with food, subject to the finished food-contact article meeting the extractive limitations under the intended conditions of use, as shown in paragraph (c) of the Regulation.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D792, ISO 1183
Melt Flow 0.70 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.70 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1183
Thermal Properties Metric English Comments
Melting Point 54.0 °C
129 °F
Freezing Point; ASTM D3417, ISO 3146
90.0 °C
194 °F
ASTM D3417, ISO 3146
Vicat Softening Point 65.0 °C
149 °F
ASTM D1525, ISO 306
Processing Properties Metric English Comments
Processing Temperature <= 285 °C
<= 545 °F
Feed Temperature 135 °C
275 °F
Blown Film Coextrusion
160 °C
320 °F
Cast Film/Sheet Processing
Zone 2 160 °C
320 °F
Blown Film Coextrusion
210 °C
410 °F
Cast Film/Sheet Processing
Zone 3 185 °C
365 °F
Blown Film Coextrusion
235 °C
455 °F
Cast Film/Sheet Processing
Zone 4 185 °C
365 °F
Blown Film Coextrusion
235 °C
455 °F
Cast Film/Sheet Processing
Zone 5 185 °C
365 °F
Blown Film Coextrusion
235 °C
455 °F
Cast Film/Sheet Processing
Adapter Temperature 185 °C
365 °F
Blown Film Coextrusion
235 °C
455 °F
Cast Film/Sheet Processing
Die Temperature 185 °C
365 °F
Blown Film Coextrusion
235 °C
455 °F
Cast Film/Sheet Processing
Melt Temperature 160 - 260 °C
320 - 500 °F