Polymer Property : Zone 2 = 275 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 2 260 - 275 °C
500 - 527 °F
Nilit Nilamid A H2 FR HF2 Unfilled, Flame Retardant PA66/6 Co-Polymer
Description: Nilamid A H2 FR HF2 is an unfilled, flame retardant NYLON 66/6 co-polymer that does not contain halogen or red phosphorous. This product combines excellent flow characteristics and extr..
Zone 2 265 - 275 °C
509 - 527 °F
Eurostar Staramide 6 70E3 PA6, 70% Mineral Filled, Injection Molded
Staramide 6 70E3 is a 70% mineral filled high density, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Zone 2 265 - 275 °C
509 - 527 °F
Eurostar Staramide PB00A PA6, 50% Glass Bead Filled, Injection Molded
Staramide PB00A is a 50% Glass Bead Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Zone 2 265 - 275 °C
509 - 527 °F
Eurostar Staramide R1000K PA66, Injection Molded
Staramide R1000K is an Unreinforced Radiation Crosslinkable Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Zone 2 265 - 275 °C
509 - 527 °F
Eurostar Staramide RF004EU PA66/6, 20% Glass Fiber Filled, Injection Molded
Staramide RF004EU is a 20% Glass Fiber Reinforced Polyamide 66/6 Injection Molding (also known as Staramide 66C 20V S4)Information provided by Eurostar.
Zone 2 265 - 275 °C
509 - 527 °F
Eurostar Starflam RF0052E PA66/6, Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam RF0052E is a Flame Retardant, Halogen Free, Red Phosphorous Free, Glass Reinforced Polyamide 66/6 Injection Molding ResinInformation provided by Eurostar.
Zone 2 265 - 275 °C
509 - 527 °F
Eurostar Starflam RFK517E PA66, Glass/Mineral Fiber Reinforced, Flame Retardant, Injection Molding
Starflam RFK517E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Mineral Filled, Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Zone 2 265 - 275 °C
509 - 527 °F
Eurostar Staramide PX05046 PA6, Glass Bead/Fiber Filled, Injection Molded
Staramide XP05046 is Glass Bead and Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Zone 2 265 - 275 °C
509 - 527 °F
Eurostar Staramide RF006EU PA66/6, Glass Fiber Filled, Injection Molded
Staramide RF006EU is an UV stabilized, Glass Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as Staramide 66C 30V S4)Information provided by Eurostar.
Zone 2 230 - 275 °C
446 - 527 °F
Ascend Performance Materials Vydyne® 75HF Nylon 66/6, Heat Stabilized, DAM
Vydyne® 75HF is a medium-high-viscosity, heat-stabilized PA66/6 copolymer resin designed for extrusion applications. It is available in natural color only. Vydyne 75HF resin offers a well-balanced ..