Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 2 | 265 - 290 °C | 509 - 554 °F | |
Nilit Nilamid A3 N H2 Nucleated, Heat Stabilized Nylon 66 Description: Nilamid A3 N H2 is a nucleated, heat stabilized NYLON 66 with excellent flow characteristics and very fast cycle time. It is widely used throughout many industries for mass production a.. |
|||
Zone 2 | 265 °C | 509 °F | |
Honeywell Aegis™ HFX High Barrier Nylon
(discontinued **) Description: Aegis® HFX is an oxygen scavenging polyamide composition formulated specifically for use in high performance packaging applications where high gas barrier is required. This product is .. |
|||
Zone 2 | 265 - 275 °C | 509 - 527 °F | |
Eurostar Staramide 6 70E3 PA6, 70% Mineral Filled, Injection Molded Staramide 6 70E3 is a 70% mineral filled high density, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 265 - 275 °C | 509 - 527 °F | |
Eurostar Staramide PB00A PA6, 50% Glass Bead Filled, Injection Molded Staramide PB00A is a 50% Glass Bead Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 265 - 275 °C | 509 - 527 °F | |
Eurostar Staramide R1000K PA66, Injection Molded Staramide R1000K is an Unreinforced Radiation Crosslinkable Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 265 - 275 °C | 509 - 527 °F | |
Eurostar Staramide RF004EU PA66/6, 20% Glass Fiber Filled, Injection Molded Staramide RF004EU is a 20% Glass Fiber Reinforced Polyamide 66/6 Injection Molding (also known as Staramide 66C 20V S4)Information provided by Eurostar. |
|||
Zone 2 | 265 - 280 °C | 509 - 536 °F | |
Eurostar Starflam AFR200Y PA66, Flame Retardant, Injection Molding Staramide AFR200Y is an Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 265 - 275 °C | 509 - 527 °F | |
Eurostar Starflam RF0052E PA66/6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam RF0052E is a Flame Retardant, Halogen Free, Red Phosphorous Free, Glass Reinforced Polyamide 66/6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 265 - 275 °C | 509 - 527 °F | |
Eurostar Starflam RFK517E PA66, Glass/Mineral Fiber Reinforced, Flame Retardant, Injection Molding Starflam RFK517E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Mineral Filled, Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 265 - 280 °C | 509 - 536 °F | |
Eurostar Starflam RX06082 PA66/6, Glass Fiber Filled, Flame Retardant, Injection Molded Staramide RX06082 is a Halogen Free and Red Phosphorous Free, flame Retardant, Glass Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 265 - 275 °C | 509 - 527 °F | |
Eurostar Staramide PX05046 PA6, Glass Bead/Fiber Filled, Injection Molded Staramide XP05046 is Glass Bead and Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 265 - 275 °C | 509 - 527 °F | |
Eurostar Staramide RF006EU PA66/6, Glass Fiber Filled, Injection Molded Staramide RF006EU is an UV stabilized, Glass Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as Staramide 66C 30V S4)Information provided by Eurostar. |
|||
Zone 2 | 265 °C | 509 °F | Compression |
BASF Ultradur® S 4090 GX 14% Glass Filled PBT Description: Is a PBT + ASA, low-warpage, free-flowing injection-molding grades with very good processing capabilities, containing 14% of glass fibers for industrial parts with high dimensional stab.. |
|||
Zone 2 | 265 °C | 509 °F | Compression |
BASF Ultradur® S 4090 G2 10% Glass Filled PBT Description: Is a PBT + ASA, easy-flowing injection-molding grades with 10% glass fibers; for rigid, tough and dimensionally stable technical parts e. g. housings, consoles, contact carriers, covers.. |
|||
Zone 2 | 265 °C | 509 °F | Compression |
BASF Ultradur® B 4040 G10 50% Glass Filled BK 15029 PBT + PET Description: Injection molding grade with 50% glass fibers for industrial parts with excellent surface quality, for example external door handles in vehicles, visible sunroof frames, oven door handl.. |
|||
Zone 2 | 265 °C | 509 °F | Compression |
BASF Ultradur® S 4090 G6X 30% Glass Filled PBT Description: Is a PBT + ASA, low-warpage, free-flowing injection-molding grades with very good processing capabilities, containing 30% of glass fibers for industrial parts with high dimensional stab.. |
|||
Zone 2 | 265 °C | 509 °F | Compression |
BASF Ultradur® B 4040 G4 20% Glass Filled PBT + PET PBT + PET, injection-molding grade containing 20% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor housin.. |
|||
Zone 2 | 265 °C | 509 °F | Compression |
BASF Ultradur® B 4040 G6 30% Glass Filled PBT + PET PBT + PET, injection-molding grade containing 30% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor housin.. |
|||
Zone 2 | 265 °C | 509 °F | Compression |
BASF Ultradur® B 4300 G10 50% Glass Filled PBT Description: Injection-molding grades containing 50% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor hou.. |