Material Notes:
Staramide R1000K is an Unreinforced Radiation Crosslinkable Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.014 - 0.016 cm/cm

@Thickness 4.00 mm
0.014 - 0.016 in/in

@Thickness 0.157 in
E2P method
Mechanical Properties Metric English Comments
Tensile Strength at Break 80.0 MPa
11600 psi
5 mm/min; ISO 527
Elongation at Break 3.0 %
3.0 %
5 mm/min; ISO 527
Flexural Strength 100 MPa
14500 psi
2 mm/min; ISO 178
Flexural Modulus 2.50 GPa
363 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
80x10x4; ISO 180/1A
Izod Impact, Unnotched (ISO) 25.0 kJ/m²
11.9 ft-lb/in²
80x10x4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 56.0 °C
133 °F
Flatw 80x10x4, sp=64 mm; ISO 75/Af
Processing Properties Metric English Comments
Zone 1 265 - 275 °C
509 - 527 °F
Zone 2 265 - 275 °C
509 - 527 °F
Zone 3 265 - 275 °C
509 - 527 °F
Melt Temperature 265 - 275 °C
509 - 527 °F
Mold Temperature 60.0 - 100 °C
140 - 212 °F
Moisture Content 0.20 %
0.20 %