Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 3 | 188 °C | 370 °F | Extrusion |
Lubrizol ESTANE® 58219 Ether Based Thermoplastic Polyurethane Features: Excellent physical properties, hydrolysis resistance, low temperature performance and clarity. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection .. |
|||
Zone 3 | 188 °C | 370 °F | Extrusion |
Lubrizol ESTANE® 58237 Ether Based Thermoplastic Polyurethane Features: High moisture vapor transmission. Good physical properties and elasticity.Uses: Blown and flat die/cast film extrusion.Available in Americas, Europe, Middle East, Africa, India and AsiaInf.. |
|||
Zone 3 | 188 °C | 370 °F | Extrusion |
Lubrizol ESTANE® 58238 Ester Based Thermoplastic Polyurethane Features: Highly Elastic Compound and Good Recovery for a Rubber-Like CharacterUses: Flat Die/Film Extrusion and Blown Film and Injection Molding and Profile ExtrusionAvailable in Americas, Europe, .. |
|||
Zone 3 | 188 °C | 370 °F | Extrusion |
Lubrizol ESTANE® 58309 Ether Based Thermoplastic Polyurethane Features: Good Physical Properties and Reduced Surface Tack.Uses: Flat Die/Cast Film and Blown Film Extrusion, Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInfo.. |
|||
Zone 3 | 188 °C | 370 °F | Extrusion |
Lubrizol ESTANE® 58370 Ether Based Thermoplastic Polyurethane Features: Halogenated flame retardant compoundUses: Extrusion – Wire and cable and general application where flame retardant properties are neededAvailable in Americas, Europe, Middle East, Africa,.. |
|||
Zone 3 | 188 °C | 370 °F | Extrusion |
Lubrizol ESTANE® 58863 Ether Based Thermoplastic Polyurethane Features: Good Elasticity – High melt flow for easy processingUses: Extrusion – Wire and cable, general extrusionAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provi.. |
|||
Zone 3 | 188 °C | 370 °F | Extrusion |
Lubrizol ESTANE® 58866 Ether Based Thermoplastic Polyurethane Features: Transparent flame retardant compoundUses: Extrusion – Wire and cable, Hose and tubeAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol. |
|||
Zone 3 | 188 °C | 370 °F | Extrusion |
Lubrizol ESTANE® 58881 Ether Based Thermoplastic Polyurethane Features: Very high tensile strength, excellent low temperature flexibility, and superior abrasion and cut resistanceUses: Extrusion – Wire and cable, Hose and tube & General purposeAvailable in Am.. |
|||
Zone 3 | 188 °C | 370 °F | Extrusion |
Lubrizol ESTANE® 58887 Ether Based Thermoplastic Polyurethane Features: Excellent hydrolysis resistance, low temperature performance, clarity and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and blow molding; cab.. |
|||
Zone 3 | 188 °C | 370 °F | Extrusion |
Lubrizol ESTANE® 58271 Ester Based Thermoplastic Polyurethane Features: Good physical properties, chemical resistance and adhesive properties and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and blow molding.Avai.. |
|||
Zone 3 | 188 °C | 370 °F | Extrusion |
Lubrizol ESTANE® 58277 Ester Based Thermoplastic Polyurethane Features: Excellent physical properties, good chemical resistance and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion and Injection and blow molding.Complies with: .. |
|||
Zone 3 | 188 °C | 370 °F | Extrusion |
Lubrizol ESTANE® 58206 Ester Based Thermoplastic Polyurethane Features: Good Flexibility at Low Temperatures and Improved Weathering Performance.Uses: Flat Die/Cast Film Extrusion and Hose/Profile Extrusion, Injection Molding.Available in Americas, Europe, Mid.. |