Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 3 | 190 - 210 °C | 374 - 410 °F | Blow Molding |
LG Chemical BM662B ABS, Heat Resistance Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 31621-07-5Information provided by LG Chemica.. |
|||
Zone 3 | 190 - 205 °C | 374 - 401 °F | Injection Molding |
Kolon ELLAS K-793AB Ester Based Thermoplastic Polyurethane ApplicationsFilm/SeatBlown filmIndustry Parts Information provided by API-Kolon. |
|||
Zone 3 | 190 °C | 374 °F | |
SK Chemicals SKYTHANE® X590A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Zone 3 | 190 °C | 374 °F | |
Lubrizol Estane® X-590A-2FR Thermoplastic Polyurethane Type: Estane® X-590A-2FR TPU is a Shore 89A, polyester type thermoplastic polyurethane elastomer.Uses: Film Blowing, Extrusion.Available in AsiaInformation Provided by The Lubrizol Corporation |
|||
Zone 3 | 190 °C | 374 °F | Extrusion |
Lubrizol Estane® ZHF 90AT0 Thermoplastic Polyurethane, Flame Retardant Type: Estane® ZHF 90AT0 TPU is a clear, glossy, zero halogen flame retardant polyether based thermoplastic polyurethane compound.Features: Outstanding TPU properties.Uses: Cable jacket and tube/hos.. |
|||
Zone 3 | 190 - 200 °C | 374 - 392 °F | |
Eurostar Starflam M10009AP PP, Flame Retardant, Injection Molding Starflam M10009AP is an Unfilled Flame Retardant high fluidity Polypropylene (Homo) Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 190 - 200 °C | 374 - 392 °F | |
Eurostar Starflam MX05075 PP, Flame Retardant, Injection Molding Starflam MX05075 is an Unfilled Halogen Free Flame Retardant PP Injection Molding ResinInformation provided by Eurostar. |