Processing Properties Metric English Comments
Zone 3 380 °C
716 °F
Victrex® PEEK 600G Polyetheretherketone  (discontinued **)
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta..
Zone 3 380 °C
716 °F
Victrex® WG101™ Polyaryletherketone
Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, black, granules for injection moulding, easy flow with wear additivesWG101 does not contai..
Zone 3 380 - 390 °C
716 - 734 °F
Lehmann & Voss LUVOCOM® 2205-7054 Blend based on polyaryl ether ketone, with glass fiber
Applications: High dimensionally stable precision parts, high continuous use temperature.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceChemical and hydr..
Zone 3 380 - 390 °C
716 - 734 °F
Lehmann & Voss LUVOCOM® 2205-7123 Blend based on polyaryl ether ketone, with carbon fiber, PTFE, lubricant modified
Applications: High dimensionally stable precision parts, high continuous use temperature.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceChemical and hydr..
Zone 3 380 - 390 °C
716 - 734 °F
Lehmann & Voss LUVOCOM® 2211-7726 Blend of polyarylate, with carbon fiber
Applications: Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High dimensionally stable precision parts.Suitable for discharging of statically generated electr..
Zone 3 380 - 390 °C
716 - 734 °F
Lehmann & Voss LUVOCOM® 2607-7921 Blend based on polyaryl ether ketone, unreinforced
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan..
Zone 3 380 - 400 °C
716 - 752 °F
Lehmann & Voss LUVOCOM® TPI-0953 Thermoplastic polyimide, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile machinery, apparatus- and precision engineering medical- and electrical enineering, aircraft- and aerospace industry.Very high continuous use and heat dist..
Zone 3 380 - 400 °C
716 - 752 °F
Lehmann & Voss LUVOCOM® TPI-8257 Thermoplastic polyimide, with carbon fiber
Applications: Automotive industry, textile machinery, apparatus- and precision engineering medical- and electrical enineering, aircraft- and aerospace industry.High-strength and high-stiff parts; lo..