Processing Properties | Metric | English | Comments |
---|---|---|---|
Gel Time | 0.000 min @Temperature 135 °C |
0.000 min @Temperature 275 °F |
0% Gel content |
Lushan Solar EVA Film Lamination, Ultra Fast Cure EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu.. |
|||
Gel Time | 0.000 min @Temperature 138 °C |
0.000 min @Temperature 280 °F |
0% Gel content |
Lushan Solar EVA Film Lamination, Ultra Fast Cure EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu.. |
|||
Gel Time | 0.000 min @Temperature 140 °C |
0.000 min @Temperature 284 °F |
0.02% Gel content |
Lushan Solar EVA Film Lamination, Ultra Fast Cure EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu.. |
|||
Gel Time | 0.000 min @Temperature 143 °C |
0.000 min @Temperature 289 °F |
0.09% Gel content |
Lushan Solar EVA Film Lamination, Ultra Fast Cure EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu.. |
|||
Gel Time | 0.000 min @Temperature 145 °C |
0.000 min @Temperature 293 °F |
0.21% Gel content |
Lushan Solar EVA Film Lamination, Ultra Fast Cure EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu.. |
|||
Gel Time | 0.000 min @Temperature 148 °C |
0.000 min @Temperature 298 °F |
1.6% Gel content |
Lushan Solar EVA Film Lamination, Ultra Fast Cure EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu.. |
|||
Gel Time | 0.000 min @Temperature 150 °C |
0.000 min @Temperature 302 °F |
3.59% Gel content |
Lushan Solar EVA Film Lamination, Ultra Fast Cure EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu.. |
|||
Gel Time | 0.000 min @Temperature 153 °C |
0.000 min @Temperature 307 °F |
42.8% Gel content |
Lushan Solar EVA Film Lamination, Ultra Fast Cure EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu.. |
|||
Gel Time | 0.000 min @Temperature 155 °C |
0.000 min @Temperature 311 °F |
61.11% Gel content |
Lushan Solar EVA Film Lamination, Ultra Fast Cure EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu.. |
|||
Gel Time | 0.000 min @Temperature 136 °C |
0.000 min @Temperature 277 °F |
0% Gel content |
Lushan Solar EVA Film Lamination, Low Temperature Ultra Fast Cure EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu.. |
|||
Gel Time | 0.000 min @Temperature 138 °C |
0.000 min @Temperature 280 °F |
0% Gel content |
Lushan Solar EVA Film Lamination, Low Temperature Ultra Fast Cure EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu.. |
|||
Gel Time | 0.000 min @Temperature 140 °C |
0.000 min @Temperature 284 °F |
4.42% Gel content |
Lushan Solar EVA Film Lamination, Low Temperature Ultra Fast Cure EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu.. |
|||
Gel Time | 0.000 min @Temperature 143 °C |
0.000 min @Temperature 289 °F |
47.33% Gel content |
Lushan Solar EVA Film Lamination, Low Temperature Ultra Fast Cure EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu.. |
|||
Gel Time | 0.000 min @Temperature 145 °C |
0.000 min @Temperature 293 °F |
51.3% Gel content |
Lushan Solar EVA Film Lamination, Low Temperature Ultra Fast Cure EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu.. |