Processing Properties Metric English Comments
Cure Time 0.250 min

@Temperature 130 °C
0.00417 hour

@Temperature 266 °F
Dow Corning 3631 PART A&B KIT
Two-part, solvent free, heat-cured liquid silicone rubber.Information provided by Dow Corning
Cure Time 0.250 min

@Temperature 232 °C
0.00417 hour

@Temperature 450 °F
3M Scotchcast™ 260 8 G Electrical Epoxy Powder Resin
3M Scotchcast Electrical Resin 260 is a widely used, well-known general purpose epoxy powder resin. A one-part, green pigmented, rapid heat-curing product, it is designed to provide a continuous, to..