Material Notes:
3M Scotchcast Electrical Resin 260 is a widely used, well-known general purpose epoxy powder resin. A one-part, green pigmented, rapid heat-curing product, it is designed to provide a continuous, tough, moisture and chemical resistant dielectric coating to a variety of substrates. Resin 260 is manufactured by a fusion blend process, insuring that each individual particle of powder contains all the components necessary to effect a complete cure and attain stated performance properties. Resin 260 is applied to an object that has been heated to a temperature above the melting point to the resin. On contact with the preheated application surface, the resin melts, flows to a controlled extent, then cures, bonding to the substrate and coalescing into a smooth, continuous, essentially uniform thick coating. It effectively coats flat surfaces and corners, as well as high points. Uses for resin 260 include moisture-proofing and insulating armatures, stators, buss bars and toroid cores.Information provided by 3M
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
cured; ASTM D794
Mechanical Properties Metric English Comments
Impact Test 11.3 J
8.33 ft-lb
12-15 mil coating 1/8" sandblasted steel panel Gardner 5/8: Radius Impact Tester
Abrasion 0.080
0.080
[g]; ASMT D4060
Electrical Properties Metric English Comments
Dielectric Strength 39.4 kV/mm
1000 kV/in
12 to 14 mil coating; ASTM D149
Processing Properties Metric English Comments
Cure Time 0.250 min

@Temperature 232 °C
0.00417 hour

@Temperature 450 °F
0.583 min

@Temperature 204 °C
0.00972 hour

@Temperature 399 °F
7.00 min

@Temperature 177 °C
0.117 hour

@Temperature 351 °F
20.0 min

@Temperature 149 °C
0.333 hour

@Temperature 300 °F
Gel Time 0.100 - Error in fixSigDigits: @digits must be between 1 and 12. @digits is: 15 min

@Temperature 193 °C
0.100 - Error in fixSigDigits: @digits must be between 1 and 12. @digits is: 15 min

@Temperature 379 °F
hot plate
Shelf Life 12.0 Month

@Temperature <=27.0 °C
12.0 Month

@Temperature <=80.6 °F
Descriptive Properties Value Comments