Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 6480 min @Temperature 10.0 °C |
108 hour @Temperature 50.0 °F |
Full Chemical |
Chesterton ARC MX1 Vertical Build Extreme Wear Compound Description: An advanced ceramic composite for the repair and protection of all metal surfaces subjected to severe erosion, abrasion and chemical attack. It is applied at a thickness of 6 mm (1/4”).. |
|||
Cure Time | 6480 min @Temperature 10.0 °C |
108 hour @Temperature 50.0 °F |
Full Chemical |
Chesterton ARC MXC Castable Extreme Wear Compound Description: An advanced ceramic composite, with flowable viscosity, for the repair and protection of all metal surfaces subjected to severe erosion, abrasion and chemical attack. It can be hand tro.. |