Polymer Property : Cure Time = 4800 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 4800 min

@Temperature 32.0 °C
80.0 hour

@Temperature 89.6 °F
Full Chemical
Chesterton ARC CS4 low-viscosity, 100% solids, barrier coating
Description: An advanced composite formulated to protect concrete surfaces from harsh chemical attack. It is normally applied at a thickness of 250-375 microns (10-15 mils) per coat in a 2 coat syst..
Cure Time 4800 min

@Temperature 16.0 °C
80.0 hour

@Temperature 60.8 °F
Full Chemical
Chesterton ARC MX1 Vertical Build Extreme Wear Compound
Description: An advanced ceramic composite for the repair and protection of all metal surfaces subjected to severe erosion, abrasion and chemical attack. It is applied at a thickness of 6 mm (1/4”)..
Cure Time 4800 min

@Temperature 16.0 °C
80.0 hour

@Temperature 60.8 °F
Full Chemical
Chesterton ARC MXC Castable Extreme Wear Compound
Description: An advanced ceramic composite, with flowable viscosity, for the repair and protection of all metal surfaces subjected to severe erosion, abrasion and chemical attack. It can be hand tro..
Cure Time 4800 min

@Temperature 32.0 °C
80.0 hour

@Temperature 89.6 °F
Full Chemical
Chesterton ARC CS2 Low-viscosity, Composite concrete primer sealer
Description: An advanced composite formulated to protect concrete surfaces from mild chemical attack. It is normally applied at a thickness of 250-375 microns (10-15 mils) per coat. Non-shrinking. 1..