Processing Properties Metric English Comments
Cure Time 480 - 540 min

@Temperature 25.0 °C
8.00 - 9.00 hour

@Temperature 77.0 °F
De-mold Time
Northstar Polymers MPP-D80B Rigid Polyurethane
MPP-D80B has a high load-bearing property at hardness 80 D Durometer. This material has a relatively slow curing pattern. Whereas many polyurethane formulations of this hardness cure very fast thus..